DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.0 MPa
3190 psi
ASTM D638
Elongation at Break 100 %
100 %
ASTM D638
Flexural Modulus 0.990 GPa
144 ksi
ASTM D790
Izod Impact, Notched 1.80 J/cm
3.37 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ASTM D648
UL RTI, Electrical 115 °C
239 °F
0.030 in; UL 94
Flammability, UL94 V-2

@Thickness 1.57 mm
V-2

@Thickness 0.0618 in
V-2

@Thickness 3.05 mm
V-2

@Thickness 0.120 in