Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.59 J/cm @Temperature -30.0 °C |
2.98 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
Izod Impact, Notched | 1.59 J/cm @Temperature -30.0 °C |
2.98 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC (Asia Pacific) design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
Izod Impact, Notched | 1.59 J/cm @Temperature -30.0 °C |
2.98 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC (Europe-Africa-Middle East) design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
Izod Impact, Notched | 1.59 J/cm | 2.98 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF00C PA 66 LNP THERMOCOMP* RF00C is a compound based on Nylon 66 resin containing 60% Glass Fiber. |
|||
Izod Impact, Notched | 1.59 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.98 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers NYLON 6630 L Black Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 1.59 J/cm | 2.98 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP 9X11427 LNP* THERMOCOMP* 9X11427 is a compound based on Miscellanbeous resin containing 40% specialty glass filled TP alloy. Added features of this grade include: Ultra-Stiff Toughness, Improved Impact, G.. |