Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.45 J/cm @Temperature -30.0 °C |
2.72 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer 18 MFR LEXAN High Flow Ductile Copolymer |
|||
Izod Impact, Notched | 1.45 J/cm @Temperature -30.0 °C |
2.72 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer (Europe-Africa-Middle East) 18 MFR LEXAN High Flow Ductile Copolymer |
|||
Izod Impact, Notched | 1.45 J/cm @Temperature -30.0 °C |
2.72 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1232 PC Copolymer 18 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only |
|||
Izod Impact, Notched | 1.45 J/cm @Temperature -30.0 °C |
2.72 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1232 PC Copolymer (Asia Pacific) 18 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only |
|||
Izod Impact, Notched | 1.45 J/cm @Temperature -30.0 °C |
2.72 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1232 PC Copolymer (Europe-Africa-Middle East) 18 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only |
|||
Izod Impact, Notched | 1.45 J/cm @Temperature -30.0 °C |
2.72 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer (Asia Pacific) 18 MFR LEXAN High Flow Ductile Copolymer |
|||
Izod Impact, Notched | 1.45 J/cm | 2.72 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DX13354 PC COPOLYMER (Asia Pacific) DX13354 is 30% glass fiber reinforced, impact modified and LDS functionalized polycarbonate resin. The features include LDS function, high flow, and good ductility. |
|||
Izod Impact, Notched | 1.45 J/cm @Temperature -30.0 °C |
2.72 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL NH5120C PPE+PS Noryl* NH5120C resin is a modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, good chemical resistance, and low specifc gravity for light weight parts. The .. |
|||
Izod Impact, Notched | 1.45 J/cm @Temperature -30.0 °C |
2.72 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL NH5120C PPE+PS (Asia Pacific) Noryl* NH5120C resin is a modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, good chemical resistance, and low specifc gravity for light weight parts. The .. |
|||
Izod Impact, Notched | 1.45 J/cm @Temperature -30.0 °C |
2.72 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL NH5120C PPE+PS (Europe-Africa-Middle East) Noryl* NH5120C resin is a modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, good chemical resistance, and low specifc gravity for light weight parts. The .. |
|||
Izod Impact, Notched | 1.45 J/cm | 2.72 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP D452 PC COPOLYMER (Asia Pacific) LNP* Thermocomp* D452 (or EXTC8202) is a compound based on SABIC unique Polycarbonate copolymer resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, .. |
|||
Izod Impact, Notched | 1.45 J/cm | 2.72 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RX99732C PA 66 LNP* Thermocomp* PDX-R-99732 is a Nylon 6/6 with proprietary fillers. |