Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.23 J/cm @Thickness 3.17 mm |
2.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Fiberfil® J-68/20/E/SD/HM Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled, with static dissipation Information provided by FIBERFIL Engineered Plastics |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
Global POM-100 High Viscosity Acetal Homopolymer Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
Ineos J50-200-178 HDPE A high density polyethylene copolymer. It has a narrow molecular weight distribution and is intended for the molding of screw caps dedicated to the packaging of carbonated beverages. This material m.. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256-A |
Ineos Styrenics Avantra® 585K Q402 Rubber Modified Polystyrene Avantra® 585K Q402 is a high-impact grade of polystyrene with extremely high surface gloss and excellent practical toughness. Although Avantra® 585K Q402 can be processed by any method applic.. |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.20 mm |
2.30 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
KKPC Kuhmo HF 430U Weather-resistant Flame Retarded HIPS Key features: Excellent weather-resistance, non-deca heat-resistance. Common Uses: TV and VCR housing, parts needing non-deca type.HIPS is a functional resin made by copolymerization of styrene mono.. |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.20 mm |
2.30 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
KKPC Kuhmo HFH 405 Flame Retarded HIPS Key features: Non-halogen type. Common Uses: Parts needing non-halogen type.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-.. |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.17 mm |
2.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PA6/6 FR HS BK (Conditioned) Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.17 mm |
2.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PA6/6 FR NAT Availability: North AmericaForms: PelletsFeatures: Flame Retardant UL File Number: E157318Appearance: Natural ColorProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.17 mm |
2.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 IM 0240 Impact Modified Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforAdditive: Impact ModifierFeatures: High Density and Impact ModifiedProcessing Method: Injection MoldingInform.. |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.17 mm |
2.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/10 GF30 L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Lubricant Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.17 mm |
2.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PP CO GF15 CC 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
Stratasys® PC-ABS PC-ABS (polycarbonate-ABS) is one of the most widely used industrial thermoplastics. PC-ABS offers the most desirable properties of both materials - the superior mechanical properties and heat resis.. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
Techmer ES Plaslube® J-4/30/TF/13/SI/2 BK223 PA6/12 |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.17 mm |
2.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® TPX-HTN-000BB Availability: North AmericaForms: Pellets Features: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.17 mm |
2.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PA6/6 GF33 FR HS L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInform.. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 1329 Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1329 is a medium impact copolymer polypropylene, available in matched automotive colors. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 6.35 mm |
2.30 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PlastxWorld CEVIAN® CGF10 10% GF PC/Acrylic Alloy Glass fiber reinforced PC/Acrylic alloy.These are typical values and are not intended for specification purposes. Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 1329 Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1329 is a medium impact copolymer polypropylene, available in matched automotive colors. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® NN230GL (DAM) Nylon 66, 33% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 1.23 J/cm @Temperature -40.0 °C |
2.30 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite Butyrate 485A2R30023 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | 1/8 in.; ASTM D256 |
Chevron Phillips EA6740 Rubber Modified Polystyrene DescriptionChevron EA6740 is a high impact polystyrene material developed for packaging applications. Its processing characteristics make EA6740 excellent for extrusion and deep-draw thermoforming... |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | injection molded; ASTM D256 |
Americas Styrenics EC6600 High Impact Polystyrene Product CharacteristicsExcellent printabilityMatte surface finishHigh heat distortion temperatureGood low temperature toughnessFood Contact CompliantTypical ApplicationsLithographic sheetPrinted toy.. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 520-40G Nylon 66, 40% Glass Reinforced A general purpose 40% glass reinforced Nylon 66 resin.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 925LMS-22G Nylon 12, 22% Glass Reinforced A 22% glass reinforced, Molybdenum disulfide filled, Nylon 12 resin for injection molding.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.17 mm |
2.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN®-V 400N ABS Heat Resistant ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 1.23 J/cm @Temperature 22.8 °C |
2.30 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Amco PRIMATOP PP CO 220-23 Impact Polypropylene Copolymer PP CO 220-23 has easy mold flow and excellent dimensional stability. Applications include closures, housewares, and small appliance applications.Former A-Top Polymers product; part of Amco product l.. |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.17 mm |
2.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Fiberfil® J-68/20/E Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.17 mm |
2.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PA6/6 GF30 FR HS L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInform.. |