Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
Nylene® 5143 MS , 43% Glass Reinforced Low Wear Nylon 6/6 Description: Nylene® 5143 MS is a 43% glass fiber reinforced, low wear nylon 6/6. MoS2 - 2%. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies .. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
Nylene® Norpex® AX30GF , 30% Glass Reinforced Polyphenylene Ether Description: Norpex® AX30GF is a 30% glass fiber reinforced Polyphenylene Ether. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric.. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Network Polymers NPP 25-1011B Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 1.12 J/cm @Temperature -30.0 °C |
2.10 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer High viscosity Proprietary Polycarbonate Ester, OSU 55/55 compliant, low smoke, flame retardant resin |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | 73°F; ASTM D256 |
Ravago Manufacturing Americas Hylon® N2015L Nylon 6 (Cond) Information provided by Ravago. |
|||
Izod Impact, Notched | 1.12 J/cm @Temperature -30.0 °C |
2.10 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® LUX1814N PC |
|||
Izod Impact, Notched | 1.12 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
2.10 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Gravi-Tech™ GRV-NP-069-BMX Nylon 12
(discontinued **) |
|||
Izod Impact, Notched | 1.12 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.10 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa FRHIPS-113 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica.. |
|||
Izod Impact, Notched | 1.12 J/cm @Diameter 3.17 mm |
2.10 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 5404 High Impact Polystyrene High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheet, Single service packagingProperties were.. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256-A |
Ineos Styrenics 473D High-Impact Polystyrene Resin (NAFTA) Description: High-impact, high-flow grade for a wide variety of applications, including appliance components, consumer electronics housings, magnetic and optical media, building and construction, pa.. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP SFL2A PA 12 (Asia Pacific) LNP* LUBRICOMP* SFL2A is a compound based on Nylon 12 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP SFL2A PA12 LNP* LUBRICOMP* SFL2A is a compound based on Nylon 12 resin containing 50% Glass Fiber, 10% PTFE. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Notched | 1.12 J/cm @Thickness 3.17 mm |
2.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® HDPE GF30 A1 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.12 J/cm @Thickness 3.17 mm |
2.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF15 IM BK 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearan.. |
|||
Izod Impact, Notched | 1.12 J/cm @Thickness 3.17 mm |
2.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PET GF55 X 55% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 55% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP AB002 ABS (Asia Pacific) LNP* Thermocomp* AB002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Bead. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D 638 |
Styrolution PS 5310 HIPS Excellent ESCRGood ToughnessMatte easily decorated finishInformation provided by Styrolution |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM Data |
Styron Pulse® 759 ABS + Polycarbonate, 15% Glass Reinforced PULSE® 759 Engineering resin is a 15% glass reinforced resin designed to provide excellent processability, high heat resistance, and practical toughness. PULSE 759 Engineering resin has been used.. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP PX87791 PA 6 LNP* THERMOCOMP* PX87791 is a compound based on Nylon 6 resin containing Proprietary Filler(s). |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
Formosa Plastics Formolene® 2510W Medium Impact Copolymer Polypropylene Impact CopolymerApplications: Trans-white battery casesFormolene 2510W is a medium impact copolymer of polypropylene characterized by its easy mold flow, physical property balance and excellent dime.. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman... |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
Westlake Plastics HIPS High Impact Polystyrene, Compression Molded Compression molded HIPS is a low cost plastic material that is easily machined and fabricated. It is frequently used for preproduction prototyping. HIPS is a FDA compliant use in food processing a.. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman... |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. .. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
Asahi Kasei Thermylene® P7-40FG-0790 40% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® D925LH-30G Nylon 12, 30% Glass Reinforced, Lubricated A 30% glass reinforced lubricated heat and light stabilized Nylon 12. Options: D925L-30G injection molding grade, without heat and light stabilizer; and D925L-30GB for injection molding, general pu.. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
Aaron Industries AAROPRENE® GFN 6033 Glass Filled Nylon 6 AAROPRENE® GFN &G/MFN 6000 Series Reinforced CompoundsColor may be specified. |