Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.15 J/cm | 13.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® MC8200 PC+ABS (Asia Pacific) |
|||
Izod Impact, Notched | 7.16 J/cm | 13.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® BFL2000B PC (Asia Pacific) Lexan BFL2000B resin is a Br- & Cl-free FR polycarbonate resin featuring high flow with balanced impact. It is available only in dark colors. |
|||
Izod Impact, Notched | >= 7.16 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 13.4 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GN1006FM PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 7.16 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 13.4 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GN1006FMR PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, Transparency, Mold ReleaseApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG.. |
|||
Izod Impact, Notched | 7.15 J/cm | 13.4 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem GM 7746 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Izod Impact, Notched | 7.15 J/cm | 13.4 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem GM 7746 A HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Izod Impact, Notched | 7.15 J/cm | 13.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRILOY D2000 PC (Asia Pacific) LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 7.15 J/cm | 13.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRILOY D2000AXH PC LNP LUBRILOY* D2000AXH is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare. |
|||
Izod Impact, Notched | 7.15 J/cm @Temperature 23.0 °C |
13.4 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubriloy D2000XXH PC LNP LUBRILOY* D2000XXH is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated, Healthcare.This data was supplied.. |
|||
Izod Impact, Notched | 7.17 J/cm | 13.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 364 PBT (Asia Pacific) Designed for outdoor telecommunications enclosure applications. |
|||
Izod Impact, Notched | 7.15 J/cm @Temperature 0.000 °C |
13.4 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® 1105 PBT+PC (Asia Pacific) PBT/PC blend, injection molding grade, non-reinforced, impact modified, excellent toughness at low temperatures, very good paintability |
|||
Izod Impact, Notched | 7.13 J/cm @Temperature 23.0 °C |
13.4 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Xylex X7509UV PC+POLYESTER (Asia Pacific) PC+POLYESTER, Transparent, UV-Stabilized,This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 7.13 J/cm @Temperature 23.0 °C |
13.4 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Xylex X7509UV PC+POLYESTER (Europe-Africa-Middle East) PC+POLYESTER, Transparent, UV-Stabilized,This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 7.13 J/cm | 13.4 ft-lb/in | ASTM D256 |
Braskem HB 0155 HDPE Blow Molding Polyethylene Applications: Large containers from 60 to 200 litersInformation provided by Braskem |