Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.920 J/cm | 1.72 ft-lb/in | ASTM D256-93a |
Multibase Multi-Flex® TPO D-6507 Multi-Flex® D 6507 is a mineral filled TPO polypropylene compound designed for applications requiring high impact and moderate stiffness.Data provided by Multibase. |
|||
Izod Impact, Notched | 0.920 J/cm | 1.72 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DX13320C PC COPOLYMER (Asia Pacific) LNP* Statkon DX13320C is ultra clean polycarbonate/carbon fiber compound with high modulus, good flow ability, easy mold release, and high level of cleanliness for the most demanding application. A .. |
|||
Izod Impact, Notched | 0.920 J/cm | 1.72 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® IQ4860HR PBT Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Izod Impact, Notched | 0.920 J/cm | 1.72 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® IQ4860HR PBT (Asia Pacific) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Izod Impact, Notched | 0.920 J/cm | 1.72 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® IQ4860HR PBT (Europe-Africa-Middle East) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Izod Impact, Notched | 0.920 J/cm | 1.72 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® SHF436HR PBT PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant. |
|||
Izod Impact, Notched | 0.920 J/cm | 1.72 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® SHF436HR PBT (Asia Pacific) PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant. |
|||
Izod Impact, Notched | 0.920 J/cm | 1.72 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® SHF436HR PBT (Europe-Africa-Middle East) PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant. |
|||
Izod Impact, Notched | 0.920 J/cm | 1.72 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP PDXE98480 PEI LNP* Thermocomp* PDXE98480 is a compound based on Polyetherimide with Proprietary Fillers. Added feature of this grade: Reinforced. |
|||
Izod Impact, Notched | 0.920 J/cm | 1.72 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RX06421S PA 66 LNP* Thermocomp* RX06421S is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched | 0.920 J/cm | 1.72 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX1340 PPE+HIPS (Asia Pacific) PPE+PS MF Filled |
|||
Izod Impact, Notched | 0.920 J/cm @Temperature -30.0 °C |
1.72 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL EXNL0357 PPE+PS |
|||
Izod Impact, Notched | 0.920 J/cm | 1.72 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 265 PPO, 20% Glass Reinforced A general purpose, 20% glass reinforced PPO resin for injection molding applications.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.920 J/cm | 1.72 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 266 PPO, 30% Glass Reinforced A general purpose, 30% glass reinforced PPO resin for injection molding applications.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.920 J/cm | 1.72 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX2907 PPE+PS (Asia Pacific) PPE+HIPS GF10% FR V-1 |