Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.641 J/cm @Thickness 6.35 mm |
1.20 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite Optix® CA - 1000 E-2 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256 |
Plaskolite West Optix® CA-1000 IG UC Clear High Impact Acrylic Resin High impact acrylic resin, injection molding and extrusion gradeApplications: A premium impact acrylic resin particularly suited for medical and food uses. This resin is suited for Gamma irradiatio.. |
|||
Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256 |
Polymer Industries Densetec PP Homopolymer Sheet Polymer Industries’ Densetec Homopolymer Polypropylene exhibits the properties of high corrosion resistance, high temperature resistance, and great tensile strength. It maintains its stiffness at e.. |
|||
Izod Impact, Notched | 0.641 J/cm @Temperature 22.8 °C |
1.20 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources NY66-G13 Nylon 66, 13% Glass Reinforced Nylon 66, 13% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Izod Impact, Notched | 0.641 J/cm @Thickness 3.18 mm |
1.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Stat-Kon® LC-1003 Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Izod Impact, Notched | 0.641 J/cm @Thickness 3.17 mm |
1.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Fiberfil® J-60/20/E8 Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Izod Impact, Notched | 0.641 J/cm @Temperature 22.8 °C |
1.20 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
LTL Color Compounds ColorRxâ„¢ PP2-1005ARX Biocompatible, Antimicrobial Polypropylene Random Copolymer A biocompatible approx. 10 melt Polypropylene random copolymer for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All information prov.. |
|||
Izod Impact, Notched | 0.640 J/cm @Temperature 23.0 °C |
1.20 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 2200N PEI (Europe-Africa-Middle East) 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 0.641 J/cm @Thickness 3.17 mm |
1.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® ABS CF10 A1 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 8015 PEI High flow Polyetherimide blend. Meets FAR 25.853 and OSU 100/100 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Izod Impact, Notched | 0.641 J/cm | 1.20 ft-lb/in | ASTM D256 |
Techmer ES Electrafil® M-2426 BK Polycarbonate |
|||
Izod Impact, Notched | 0.641 J/cm @Thickness 3.17 mm |
1.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PET GF15 FR 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.641 J/cm @Thickness 3.17 mm |
1.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF20 HS BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Izod Impact, Notched | 0.641 J/cm @Temperature 22.8 °C |
1.20 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Teknor Apex Chemlon® 100 W Nylon 66, Unreinforced Notes: MoS2 modified; Molybdenum disulphide modified to provide self-lubrication and low friction to parts subjected to wear and abrasion. FMVSS Flammability: Passes, FMVSS 302Processing Method: Inj.. |
|||
Izod Impact, Notched | 0.641 J/cm | 1.20 ft-lb/in | ASTM D256 |
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.641 J/cm | 1.20 ft-lb/in | ASTM D256 |
A. Schulman SCHULAMID® 66 GF33H 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.641 J/cm @Thickness 3.17 mm |
1.20 ft-lb/in @Thickness 0.125 in |
injection molded sample; ASTM D256 |
American Polymers API 500 Polystyrene API 500 is a heat resistant grade of impact polystyrene. It has superior heat resistance, good impact resistance and easy colorability.Applications: API 500 is used in housewares, toys, containers,.. |
|||
Izod Impact, Notched | 0.641 J/cm | 1.20 ft-lb/in | ASTM D256A |
ExxonMobil PP9074MED Polypropylene Homopolymer Product Description: A highly clarified random copolymer resin designed for injection molding of medical devices suitable for sterilization by high energy radiation.Availability: Europe and North A.. |
|||
Izod Impact, Notched | 0.641 J/cm @Temperature 22.8 °C |
1.20 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 0.641 J/cm | 1.20 ft-lb/in | ASTM D256 |
Aaron Industries AAROPRENE® GFPP 2030 Glass Filled Polypropylene AAROPRENE® GFPP 2000 Series Glass Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Izod Impact, Notched | 0.641 J/cm @Temperature 23.0 °C |
1.20 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Formosa Plastics Formolene® 6375N Impact Copolymer Polypropylene Impact Copolymer For High Speed Injection Molded Applications Formolene® 6375N is a very high melt flow, low impact copolymer of polypropylene. It is designed for such applications as packaging, ho.. |