Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.267 J/cm @Temperature 23.0 °C |
0.500 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products P107-00 Polypropylene Homopolymer, Natural Applications: Wire harnessesTrim componentsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.267 J/cm @Temperature 23.0 °C |
0.500 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products T20P100-517UV 20% Talc Reinforced Polypropylene, UV Stabilized, Interior DX9 Black Applications: Center consolesIP componentsClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | ASTM D256 |
Network Polymers NPP 30-1200 TF40 Description: 40% Talc Filled Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 0.267 J/cm @Temperature 22.8 °C |
0.500 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources TP-FRG7.5 Polybutylene Terephthalate, 7 1/2 % Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 7 1/2 % Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Izod Impact, Notched | 0.267 - 0.801 J/cm | 0.500 - 1.50 ft-lb/in | Average value: 0.617 J/cm Grade Count:14 |
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl.. |
|||
Izod Impact, Notched | 0.267 - 7.47 J/cm | 0.500 - 14.0 ft-lb/in | Average value: 2.11 J/cm Grade Count:18 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | ASTM D256 |
Global TPP-110 10% Talc Filled Polypropylene Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | ASTM D256 |
Global TPP-120 20% Talc Filled Polypropylene Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 0.267 J/cm @Thickness 3.17 mm |
0.500 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® HDPE TM5 5% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 5% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | ASTM D256 |
A. Schulman PP 3476 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided .. |
|||
Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | ASTM D256 |
A. Schulman PP 3488-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3488-01 is a specially formulated homopolymer polypropylene designed for large appliance injection molding. This material has excellent chemical resistance in addition t.. |
|||
Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | at 0°F; ASTM D256 |
A. Schulman PP 1116-01 Polypropylene Molding Grade Copolymer Polypropylene DescriptionPolypropylene PP 1116-01 is a molding grade copolymer polypropylene with improved low temperature toughness and good room temperature toughness. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | ASTM D256 |
A. Schulman PP 3487-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3487-01 is a special homopolymer polypropylene formulated with a long term heat aging resistance. This material has excellent resistance to chemicals and solvents. High.. |
|||
Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | ASTM D256 |
A. Schulman PP 3490-01G Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3490-01G Natural is a homopolymer for extrusion and compounding applications. This material can also be used as a carrier resin for color concentrates. ApplicationPP 349.. |
|||
Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | ASTM D256 |
A. Schulman PP 1102-01 Polypropylene General Purpose, Molding Grade Polypropylene DescriptionPolypropylene PP 1102-01 is a general purpose, molding grade with UL 94 HB approval for use in large and thin wall applications. ApplicationPolypropylene PP 1102-01 meets FDA Regulation.. |
|||
Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | ASTM D256 |
Formosa Plastics Formolene® 4142T Injection Molding Polypropylene Homopolymer with Nucleating, Antistat AdditivesApplications: Appliance, closure and thin wall applications.Formolene 4142T is a low viscosity, highly isotactic polypropylene homopolymer designed pri.. |
|||
Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | ASTM D256 |
A. Schulman PP 3490-01G Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3490-01G Natural is a homopolymer for extrusion and compounding applications. This material can also be used as a carrier resin for color concentrates. ApplicationPP 349.. |
|||
Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | |
Tra-Con Tra-Bond 2211 High Temperature Epoxy Adhesive TRA-BOND 2211 is a low viscosity epoxy adhesive system recommended for industrial bonding applications where superior wetting and good mechanical and electrical insulation performance features are r.. |
|||
Izod Impact, Notched | 0.267 J/cm @Temperature 22.8 °C |
0.500 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Amco PRIMATOP PP HOMO 350NA Injection Molding Polypropylene Features:nucleationanti-statlow viscosityexcellent processabilityexcellent stiffnessminimal odor or tasteApplications:thin wall partsclosuressmall appliancesFormer A-Top Polymers product; part of Am.. |
|||
Izod Impact, Notched | 0.267 J/cm @Thickness 3.17 mm |
0.500 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall 3802 Vinyl Foam, Extrusion Georgia Gulf 3801, 3802, and 3803 are vinyl foam compounds designed for applications requiring lower density than standard rigid vinyls.Information provided by Georgia GulfGeorgia Gulf became Axiall.. |
|||
Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | At 73°F; ASTM D256 |
Plastics Group Polifil® T-30 30% Talc-Reinforced Polypropylene Polifil® T series compounds are homopolymer polypropylene resins reinforced with asbestos-free talc. They possess high flex modulus, high deflection temperature, good chemical resistance and colora.. |
|||
Izod Impact, Notched | 0.267 J/cm @Temperature 23.0 °C |
0.500 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products CC30P100-00 30% Calcium Carbonate Reinforced Polypropylene, Natural Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | ASTM D256 |
Amco Amalloy® B9575 Polymer Alloy Amco Amalloy B9575 is a clear performance copolymer with exceptional clarity and toughness.Very clear, high tensile and flexural strength.Information provided by Amco Plastic Materials. |