Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.427 - 8.00 J/cm | 0.800 - 15.0 ft-lb/in | Average value: 1.34 J/cm Grade Count:102 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Izod Impact, Notched | 1.15 - 8.00 J/cm | 2.15 - 15.0 ft-lb/in | Average value: 4.92 J/cm Grade Count:3 |
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m.. |
|||
Izod Impact, Notched | 6.00 - 8.00 J/cm | 11.2 - 15.0 ft-lb/in | ASTM D256 |
Loxim 100 00V0 Polycarbonate, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 6.00 - 8.00 J/cm | 11.2 - 15.0 ft-lb/in | ASTM D256 |
Loxim 100 00V2 Polycarbonate, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 6.00 - 8.00 J/cm @Temperature 23.0 °C |
11.2 - 15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Loxim 600 00HB Polycarbonate/Polybutylene Terephthalate Information provided by Loxim Industries |