Mechanical Properties Metric English Comments
Izod Impact, Notched 0.523 - 1.12 J/cm
0.980 - 2.10 ft-lb/in
Average value: 0.733 J/cm Grade Count:8
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled". Specific grades with glass content betwe..
Izod Impact, Notched 0.600 - 1.12 J/cm

@Temperature -30.0 - -30.0 °C
1.12 - 2.10 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 0.864 J/cm Grade Count:9
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..
Izod Impact, Notched 0.534 - 1.12 J/cm
1.00 - 2.10 ft-lb/in
Average value: 0.798 J/cm Grade Count:6
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..
Izod Impact, Notched 0.883 - 1.12 J/cm
1.65 - 2.10 ft-lb/in
Average value: 0.970 J/cm Grade Count:3
Overview of materials for Thermoplastic Polyimide, Unfilled
Izod Impact, Notched 0.320 - 1.12 J/cm
0.600 - 2.10 ft-lb/in
Average value: 0.767 J/cm Grade Count:8
Overview of materials for Nylon 66, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate..
Izod Impact, Notched 0.530 - 1.12 J/cm
0.993 - 2.10 ft-lb/in
Average value: 0.793 J/cm Grade Count:14
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is ..
Izod Impact, Notched 1.01 - 1.12 J/cm
1.90 - 2.10 ft-lb/in
Average value: 1.07 J/cm Grade Count:3
Overview of materials for Polyethylene Terephthalate (PET), 60% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 60% Glass Reinforced". Specific grades with glass content between 55% ..
Copyright © lookpolymers.com All Rights Reserved