Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.00 - 1.10 J/cm | 1.87 - 2.06 ft-lb/in | Average value: 1.03 J/cm Grade Count:3 |
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled". Each property range of values reported .. |
|||
Izod Impact, Notched | 0.320 - 1.10 J/cm | 0.600 - 2.06 ft-lb/in | Average value: 0.618 J/cm Grade Count:4 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 1.10 - 1.10 J/cm @Temperature -40.0 - -40.0 °C |
2.06 - 2.06 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 1.10 J/cm Grade Count:1 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. .. |
|||
Izod Impact, Notched | 0.700 - 1.10 J/cm @Temperature -40.0 - 0.000 °C |
1.31 - 2.06 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 0.945 J/cm Grade Count:2 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Izod Impact, Notched | 0.700 - 1.10 J/cm @Thickness 3.20 - 3.20 mm |
1.31 - 2.06 ft-lb/in @Thickness 0.126 - 0.126 in |
Average value: 0.945 J/cm Grade Count:2 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Izod Impact, Notched | 0.196 - 1.10 J/cm | 0.367 - 2.06 ft-lb/in | Average value: 0.552 J/cm Grade Count:22 |
Overview of materials for Nylon 66, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu.. |
|||
Izod Impact, Notched | 0.210 - 1.10 J/cm @Temperature -40.0 - -20.0 °C |
0.393 - 2.06 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.410 J/cm Grade Count:5 |
Overview of materials for Nylon 12 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en.. |
|||
Izod Impact, Notched | 0.700 - 1.10 J/cm @Temperature -40.0 - -40.0 °C |
1.31 - 2.06 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.900 J/cm Grade Count:2 |
Overview of materials for High Density Polyethylene (HDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim.. |
|||
Izod Impact, Notched | 0.340 - 1.10 J/cm | 0.637 - 2.06 ft-lb/in | Average value: 0.728 J/cm Grade Count:5 |
Overview of materials for Acrylic, Impact Modified Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified Sheet". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 0.149 - 1.10 J/cm | 0.280 - 2.06 ft-lb/in | Average value: 0.425 J/cm Grade Count:7 |
Overview of materials for Acrylic, Optical Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr.. |