Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.374 - 1.01 J/cm | 0.700 - 1.90 ft-lb/in | Average value: 0.676 J/cm Grade Count:24 |
Overview of materials for ABS/Polyester Alloy + GF This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy + GF". Each property range of values reported is minimum and maximum values of appro.. |
|||
Izod Impact, Notched | 0.640 - 1.01 J/cm @Thickness 6.35 mm |
1.20 - 1.89 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Lubri-Tech™ MP-000/15T Modified PPO - 15% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.850 - 1.01 J/cm @Temperature -40.0 - -40.0 °C |
1.59 - 1.89 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.930 J/cm Grade Count:2 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |