Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.430 - 0.640 J/cm @Thickness 6.35 mm |
0.806 - 1.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Lubri-Tech™ AT-000/08T Acetal - 8% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.374 - 0.640 J/cm | 0.700 - 1.20 ft-lb/in | Average value: 0.485 J/cm Grade Count:11 |
Overview of materials for Nylon 612, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 0.430 - 0.640 J/cm @Thickness 6.35 mm |
0.806 - 1.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Lubri-Tech™ NL-15KV/05M Nylon 6/12 - 15% Kevlar Fiber - 5% MoS2
(discontinued **) Data provided by PolyOne. |