Polymer Property : Izod Impact, Notched = 0.350 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.250 - 0.350 J/cm
0.468 - 0.656 ft-lb/in
ASTM D256-06
Proto3000 Objet Digital Materials™ DM_8425 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide..
Izod Impact, Notched 0.220 - 0.350 J/cm
0.412 - 0.656 ft-lb/in
ASTM D256-06
Proto3000 Objet Digital Materials™ DM_8505Gray20 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr..
Izod Impact, Notched 0.220 - 0.350 J/cm
0.412 - 0.656 ft-lb/in
ASTM D256-06
Proto3000 Objet Digital Materials™ DM_8505Gray25 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr..
Izod Impact, Notched 0.220 - 0.350 J/cm
0.412 - 0.656 ft-lb/in
ASTM D256-06
Proto3000 Objet Digital Materials™ DM_8505Gray35 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr..
Izod Impact, Notched 0.220 - 0.350 J/cm
0.412 - 0.656 ft-lb/in
ASTM D256-06
Proto3000 Objet Digital Materials™ DM_8505Gray40 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr..
Izod Impact, Notched 0.250 - 0.350 J/cm
0.468 - 0.656 ft-lb/in
ASTM D256-06
Proto3000 Objet Digital Materials™ DM_8505Gray50 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr..
Izod Impact, Notched 0.350 - 0.350 J/cm

@Temperature -40.0 - -20.0 °C
0.656 - 0.656 ft-lb/in

@Temperature -40.0 - -4.00 °F
Average value: 0.350 J/cm Grade Count:1
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
Izod Impact, Notched 0.300 - 0.350 J/cm
0.562 - 0.656 ft-lb/in
ASTM D256
Loxim 300 00HB Nylon 6
Information provided by Loxim Industries
Izod Impact, Notched 0.250 - 0.350 J/cm
0.468 - 0.656 ft-lb/in
ASTM D256
Loxim 830 02C HB Polypropylene Compound, 30% Calcite Filled, Flame Retardant
Information provided by Loxim Industries
Izod Impact, Notched 0.300 - 0.350 J/cm
0.562 - 0.656 ft-lb/in
UV Postcure; ASTM D256A
DSM Somos® NeXt LV Grey
The second member of the Somos® NeXt family, Somos® NeXt LV Grey delivers the durability and functionality, with a finer resolution of details and faster part processing. This third-generation, hi..
Izod Impact, Notched 0.250 - 0.350 J/cm
0.468 - 0.656 ft-lb/in
IS 13411-1992
Amity Thermosets ATO 176 Phenolic Molding Organic and inorganic Filler, Compression Molded
Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackMedium flow App..
Izod Impact, Notched 0.220 - 0.350 J/cm
0.412 - 0.656 ft-lb/in
IS 13411-1992
Amity Thermosets AMP 481 Phenolic Molding Organic and inorganic Filler, Compression Molded
Characteristics:Good tracking resistanceGood dielectric strengthGood electrical insulation Applications:Switchgear components which ought to have high tracking resistanceCircuit protecting switche..
Izod Impact, Notched 0.350 - 0.350 J/cm

@Temperature -40.0 - -20.0 °C
0.656 - 0.656 ft-lb/in

@Temperature -40.0 - -4.00 °F
Average value: 0.350 J/cm Grade Count:1
Overview of materials for Nylon 6, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria..