Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Novablend™ 6602 Polyvinyl Chloride, Rigid (PVC, Rigid) Novablend 6602 is a rigid, opaque PVC for molding compounds. This product has high impact, excellent indoor/outdoor weathering, high flow, and good processing characteristics.Applications includes: .. |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS (Asia Pacific) PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 920 PC (Asia Pacific) Opaque colors, low viscosity, superior flame retardance. |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 920A PC Low viscosity injection moldable, flame retardant PC. Exceptional surface appearance. Clear, tints and opaque colors. |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 923A PC Low viscosity, flame retardant with exceptional surface. Clear, tints and opaque colors. UV-stabilized. |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 950 PC Opaque colors, high viscosity, superior flame retardance. |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EM3110 PC Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. |
|||
Izod Impact, Notched | 6.40 J/cm @Thickness 6.40 mm |
12.0 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer (Asia Pacific) Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in .. |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HF1140R PC (Asia Pacific) LEXAN HF1140R is a high flow grade. This material is especially designed for applications that require thin wall sections and high flow lengths. FDA food contact compliant in limited colors. Effe.. |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LUX2619 PC (Europe-Africa-Middle East) Lexan* LUX2619 Polycarbonate resin is an extrusion grade. It is UL94 V-2 rated at 1.5 mm. It was designed for high light reflectance. |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® PC2200R PC (Asia Pacific) PC2200R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® C1110HF PC+ABS High impact and ductility at 73F and -20F. For thin-wall applications. |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 940A PC Medium viscosity, flame retardant PC. Exceptional surface. Clear, tints and opaque colors. |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 943A PC (Asia Pacific) Medium viscosity, superior flame retardance. UV-Stabilized. Clear, tints and opaque colors. |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 953 PC Opaque colors, high viscosity, superior flame retardance. UV-stabilized. |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HP1 PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | edgewise; ASTM D256 |
Haysite 270FRII Polyester BMC, Glass Reinforced Haysite Grade 270FRII is a second generation glass reinforced thermoset polyester bulk molding compound. This material can be compression, transfer, or injection molded. Qualified under MIL-M-14, Ty.. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics PC2200R PC PC2200R resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplied by S.. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics PC2203R PC PC2203R resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli.. |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics PC2800 PC (Europe-Africa-Middle East) PC2800 resin is a high flow (MFR = 28 at 300°C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release... |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature -30.0 °C |
12.0 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® 1102 PBT+PC Unreinforced PC/polyester alloy. Excellent low temperatue impact/chemical resistance to automotive fluids. |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-LOY N30009 PC+ABS (Asia Pacific) LNP* Stat-loy* N30009 is a compound based on PC+ABS Blend resin containing Flame Retardant, Anti-Static. Added features of this material include: Antistat, Flame Retardant. |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-LOY NX03583 PC+ABS (Asia Pacific) LNP STAT-LOY* NX03583 is a compound based on PC+ABS Blend resin containing Anti-Static, Flame Retardant. Added features of this material include: Antistat. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature -20.0 °C |
12.0 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Asia Pacific) PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature -20.0 °C |
12.0 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Europe-Africa-Middle East) PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 7001 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 6.40 J/cm @Thickness 3.20 mm |
12.0 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Makrolon® 2205 Polycarbonate, Injection Grade Exceptionally good flow injection molding grade with easy mold release, for parts with a low wall thickness and long flow paths.Information provided by Bayer.As of 1 September 2015, Bayer MaterialSc.. |
|||
Izod Impact, Notched | 6.40 J/cm @Thickness 3.17 mm |
12.0 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® 8254 HS BK-102 PA6 (Dry) Ultramid 8254 HS is a highly flexible, heat stabilized, impact modified nylon 6 extrusion grade for tubing applications. |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 950 PC (Asia Pacific) Opaque colors, high viscosity, superior flame retardance. |
|||
Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HPH4504H PPC High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |