Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.74 J/cm @Temperature 23.0 °C |
7.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT7016-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 3.74 J/cm @Temperature 23.0 °C |
7.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT7016-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 3.74 J/cm @Temperature 23.0 °C |
7.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT7016-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D-256 |
PlastiComp Complet® LGF60 - PA6 Nylon 6, 60% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 60% long glass reinforcementInformation provided by PlastiComp, Inc. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | ASTM D256 |
Polymer Resources PPX-FR1-[color]EN Modified PPO, UL 94 V-0 with HDT of 190 F, Extrusion Grade Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Izod Impact, Notched | 3.74 J/cm @Temperature -40.0 °C |
7.00 ft-lb/in @Temperature -40.0 °F |
0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hylex® P1018LLT Polycarbonate Information provided by Ravago. |
|||
Izod Impact, Notched | 3.74 J/cm @Temperature -30.0 °C |
7.00 ft-lb/in @Temperature -22.0 °F |
0.125in; ASTM D256 |
Ravago Manufacturing Americas Hylex® P1318LLT Polycarbonate Information provided by Ravago. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D-256 |
PlastiComp Complet® LGF40-PA12 Nylon 12, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 12 with 40% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | ASTM D256 |
Global ABS-704 General Purpose High Impact ABS Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 3.74 J/cm @Thickness 3.17 mm |
7.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF50 IM2 L 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Impact Modified and LubricantFeatures: Impact Modified and LubricatedProcessin.. |
|||
Izod Impact, Notched | 3.74 J/cm @Thickness 3.17 mm |
7.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® PA6/6,6 IM 6040 BK MB Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedAppearance: BlackProcessing Metho.. |
|||
Izod Impact, Notched | 3.74 J/cm @Temperature -30.0 °C |
7.00 ft-lb/in @Temperature -22.0 °F |
0.125 in; 10 mil notch; ASTM D256 |
Styron CALIBREâ„¢ IM 401-18 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM Data |
Styron Pulse® 600 ABS + Polycarbonate PULSE® 600 Engineering resin is designed to offer a superior balance of properties between impact strength, heat resistance and processability. It offers excellent processability, medium heat res.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | -22°F; ASTM D256 |
Styron EMERGEâ„¢ 4410-18 MFR Polycarbonate EMERGEâ„¢ PC 4410-18 advanced resin is a high impact polycarbonate resin designed for Information Technology Equipment and Injection Molding Applications.Information provided by DowThis product l.. |
|||
Izod Impact, Notched | 3.74 - 5.34 J/cm | 7.00 - 10.0 ft-lb/in | |
Bulk Molding Compounds BMC 850 Corrosion Resistant, Flame Retardant Molding Compound BMC 850 is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications a.. |
|||
Izod Impact, Notched | 3.74 - 4.81 J/cm | 7.00 - 9.00 ft-lb/in | |
Bulk Molding Compounds BMC 5209-12940 Mineral Filled, Glass Reinforced Polyester BMC 5209-12940 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | ASTM D628 |
ACC EP QS EPI Engineered Polymers Quick Set Epoxy EP QS Quick Set Epoxy, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC, self-leveling modified epoxy. This versatile new generation epoxy displays low blush, fast cure.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B908 , 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 3.74 J/cm @Thickness 3.17 mm |
7.01 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PolyOne Elastamax XL-0257-2 TPU-Based Thermoplastic Elastomer
(discontinued **) This is a general purpose thermoplastic elastomer based on TPU for injection molding, and has a high specific gravity for applications requiring high weight. Physical Form: Pellets. Standard Color.. |
|||
Izod Impact, Notched | 3.74 J/cm @Temperature 23.0 °C |
7.01 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Kleerdex Kydex® 107 Acrylic/PVC Thermoplastic Sheet
(discontinued **) High performance sheet for NSFApplications: Ice makers, vending machines, beverage dispensers, and other equipment requiring NSF approval, as a replacement for stainless steel parts where cost, weig.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | Partial Break; ASTM D256 |
Ineos HB111R Polyethylene Copolymer HB111R is a natural high molecular weight, high-density copolymer polyethylene developed for automotive fuel tanks. It combines excellent processability and outstanding physical performance, particu.. |
|||
Izod Impact, Notched | 3.74 J/cm @Temperature 22.8 °C |
7.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
LTL Color Compounds ColorFast® GPA300 ABS Super-tough ABS with our highest impact strength, injection moldingAll information provided by LTL Color Compounders, Inc. |
|||
Izod Impact, Notched | 3.74 - 13.9 J/cm @Temperature -50.0 - -50.0 °C |
7.01 - 26.0 ft-lb/in @Temperature -58.0 - -58.0 °F |
Average value: 8.37 J/cm Grade Count:3 |
Overview of materials for ABS/Polyurethane Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyurethane Alloy". Each property range of values reported is minimum and maximum values of appropr.. |