Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | ASTM D256 |
PlastiComp Complet® LCF50-PA66 50% Long Carbon Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | ASTM D-256 |
PlastiComp Velocity® LGF50-PA6 High Flow Nylon 6, 50% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.50 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hylac® HF96 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.17 mm |
5.51 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Trilac® ABS-MP1000 Metal Plating Grade ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | ASTM D-256 |
PlastiComp Complet® LCF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 40% carbon fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.50 ft-lb/in | |
MTI ThermoStran® PP-50G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.50 ft-lb/in | ASTM D256 |
Multibase Multi-Flamâ„¢ 0501 PP Polypropylene Features:Flame RetardantHalogen Content, Low to None Forms:PelletsProcessing Methods:Injection MoldingExtrusionCoextrusionBlow MoldingUses:TubingPipingInformation provided by Multibase |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL STN15 PPE+HIPS (Asia Pacific) PPE+HIPS Unfilled Auto Interior |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.17 mm |
5.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 LGF50 HS L BK 12 mm Availability: North AmericaForms: PelletsFiller/Reinforcement: Long Glass FiberAdditive: Lubricant and Heat StabilizerFeatures: Lubricated, Heat Stabilized and Good MoldabilityUL File Number: E15731.. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | |
Shinil Chemical SHINFLAME PC/ABS Flame Retardant Polymer TV Housing SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to prod.. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.50 ft-lb/in | |
Saint-Gobain Rulon® DC1042 Bearing/Seal PTFE Can be used in a wide range of sealing and bearing applications. Rulon DC1042 is ideal for applications in which the bearing, seal is in contact with harsh chemicals or in applications where electri.. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.17 mm |
5.51 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® GC-0703 ABS/PET, Unreinforced Recycled Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.17 mm |
5.51 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® GC-0703 ABS/PET, Unreinforced Recycled Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.17 mm |
5.51 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® SR-7300 ABS/PET, Unreinforced Material with superior chemical resistance that can be used in the interior/exterior material of household appliances that require heat resistanceInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | ASTM Data |
Styron Magnum™ 2620 ABS, Impact Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Izod Impact, Notched | 2.94 J/cm @Temperature 23.0 °C |
5.51 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl EBN9003 PPE+HIPS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | |
Zylog Hipolyene® 1532 MS Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.50 ft-lb/in | ASTM D256 |
Total HDPE BM962 High Density Polyethylene, High Gloss Blow Molding Resin Polyethylene: High density High Gloss Blow Molding ResinCharacteristics:High GlossHigh stiffnessGood abrasion resistanceFDA CompliantApplications:Coextruded glossy bottlesBlending agent for other p.. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
5.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 3501 Natural 1050 Description: Natural, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
5.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 3502 Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
5.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 3502E Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | ASTM Data |
Dow AIM® 4800 High Impact Styrenic Resin AIM® 4800 advanced styrenic resin is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss ABS. It can be processed at lower temperatur.. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.50 ft-lb/in | ASTM D256A |
Dow INSPIRE™ D560.00 Developmental Performance Polymer D 560.00 Performance Polymer has consistent processability, high gloss, good regrind stability, and contains U.V. stabilizers for increased weatherability. D 560.00 Performance Polymer is intended f.. |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® ABS Resin F-216 General purpose high impact resin.Data provided by the manufacturer |
|||
Izod Impact, Notched | 2.94 J/cm | 5.51 ft-lb/in | ASTM Data |
Styron Magnum™ 9025 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |