Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 1.08 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
Polimersan Plastics POLITEF® (PTFE) with 60% Bronze
As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv..
Izod Impact, Notched 1.08 J/cm

@Temperature -30.0 °C
2.02 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Europe-Africa-Middle East)
55 MFR LEXAN High Flow Ductile Copolymer, Natural color only
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
Polimersan Plastics POLITEF® (PTFE) with 60% Bronze
As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv..
Izod Impact, Notched 1.08 J/cm

@Temperature -30.0 °C
2.02 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer
55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only
Izod Impact, Notched 1.08 J/cm

@Temperature -30.0 °C
2.02 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer (Europe-Africa-Middle East)
55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® SLDM310 PC (Asia Pacific)
Mineral filled Antistatic Polycarbonate, HDT110degC type
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
Mitsui AURUM® JCL3030 Thermoplastic Polyimide Resin, Amorphous, Wear/Friction Grade  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
Izod Impact, Notched 1.08 - 1.40 J/cm
2.02 - 2.62 ft-lb/in
Average value: 1.29 J/cm Grade Count:4
Overview of materials for Polytetrafluoroethylene (PTFE), Bronze Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Bronze Filled". Each property range of values reported is minimum and ma..
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
Kolon KOPA® KN333G30BL G/F Reinforced Nylon 66
G/F 30% reinforcedApplications Engine coversInformation provided by API-Kolon.
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
Kolon KOPA® KN333G30CRN G/F Reinforced Nylon 66
Oil resistantApplications Surge tanksInformation provided by API-Kolon.
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
DIN 53453; ASTM D256
Kolon KOPA® KN333G33CR G/F Reinforced Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
Izod Impact, Notched 1.08 J/cm

@Temperature 23.0 °C
2.02 ft-lb/in

@Temperature 73.4 °F
ASTM D256
LG Chemical LUPOY GP-2301F General Purpose Modified PC, 30% Glass Fiber Reinforced, Flame Retardant
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Izod Impact, Notched 1.08 J/cm

@Temperature 23.0 °C
2.02 ft-lb/in

@Temperature 73.4 °F
ASTM D256
LG Chemical SEETEC T3410 Polypropylene Random Terpolymer
Features: Seetec T3410 is a polypropylene-ethylene-butene random terpolymer designed for the production of Transparent Film and Expandable PP for low seal temperature and high impact strength. It of..
Izod Impact, Notched >= 1.08 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
>= 2.02 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUPOY GN2201FM PC+GF20%, Halogen Free, Flame Retardant, Heat Resistance
Description: Injection Molding, PC+GF20%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov..
Izod Impact, Notched 1.08 J/cm

@Temperature 23.0 °C
2.02 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Valox® PDR4911 PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
Shinil Chemical SHINSTRA PA-6 AG30N Structural Polymer Wheel Cover
SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog..
Izod Impact, Notched 1.08 J/cm

@Thickness 3.17 mm
2.02 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® GP-8300G MPPE, 30% Glass Filled
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 1.08 J/cm

@Thickness 3.17 mm
2.02 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® HR-8070 MPPE, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 1.08 J/cm

@Thickness 3.17 mm
2.02 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® NH-3402F PC, 40% Glass Filled FR
PC/GF material with 40% GF reinforcement that can be used in printer LSUInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 1.08 J/cm

@Thickness 3.17 mm
2.02 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® SF-0950S MABS, Unreinforced Scratch Resistant
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 1.08 J/cm

@Thickness 3.17 mm
2.02 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® GP-8300G MPPE, 30% Glass Filled
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL GFN1740V PPE+PS
Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Europe-Africa-Middle East)
Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
Cheng Yu Plastic ML848 Flame Retardant PC
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
Cheng Yu Plastic T881 Flame Retardant PBT
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
Cheng Yu Plastic T889G25 PBT, 25% Glass Fiber
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
E-Polymers TEKAPPO® J920 20% Glass Fiber Reinforced M-PPO
Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a..
Izod Impact, Notched 1.08 J/cm

@Thickness 3.17 mm
2.02 ft-lb/in

@Thickness 0.125 in
ASTM D256
Unitika U-8000
U series resins are polymer alloys that are improved in resistance to oils and chemicals, the shortcoming of amorphous resins. They are transparent and have a greater moisture blocking property than..
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
Zylog Hipolyene® 4955 T Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
Plenco 50045 PET, Pellet, Injection Molded, Natural Color  (discontinued **)
PLENCO 50045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is UL listed and available in white, natural, and black.Information s..