Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_8320 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide.. |
|||
Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP KONDUIT PX10322 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compound, with through-plane and in-plane thermal conductivity of 1.7 W/(m*K) and 4.7 W/(m*K) respectively, conforming to ASTM E 1461 test standard. |
|||
Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | ASTM D256A |
Total Finaclear® 530 Clear Impact Polystyrene
(discontinued **) Finaclear® 530 is a clear high styrenic styrene-butadiene (SBS) elastomer, providing dramatically improved impact properties and tear resistance to finished articles, when used in blends with other.. |
|||
Izod Impact, Notched | 0.200 J/cm @Diameter 3.17 mm |
0.375 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 2510 General Purpose Crystal Polystyrene
(discontinued **) High speed molding, Improved crack resistance, USP Class VIApplications: Cutlery, Light louvers, RazorsExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the phy.. |
|||
Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | ASTM D256 |
Ineos Nova 50 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High strength crystal polystyrene, High heat crystal polystyrene, Custom colorsApplications: Injection molding or extrusion, Designed for applications requiring strength and high heat resistance whe.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar |
BP Amoco Amoco® 7644 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Consumer products, CompoundingComplies with FDA specification, Title 21, CFR 177.1520.Typical property .. |
|||
Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | 23° C; ASTM D256 |
Flint Hills P4C5Z-027 Homopolymer Polypropylene Homopolymer, UL certified, USP Class VI certified, and FDA compliant.Features: controlled rheology.Applications: Injection molding: general purpose.Former Huntsman polypropylene products are now pro.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H03G-00 Polypropylene Homopolymer Suggested fabrication methods: ExtrusionFeatures: Low water carry-overTypical applications: Woven fabric, Cordage, Slit filmComplies with FDA specification, Title 21, CFR 177.1520.Typical property d.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H20H-00 Polypropylene Homopolymer This resin is designed to provide easy moldability for applications requiring resistance to long term heating. This material has been recognized by UL for sustained use at 130c.Suggested fabricatio.. |
|||
Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | ASTM D256 |
SPS Guang Zhou SAMATâ„¢ EP 5001(f1) Flame-retarded Polypropylene Characteristic: Good flame retardance, non-halogen, high flow properties, high rigidity, high heat resistance, meets the requirements of RoHs and PaHs, excellent UV resistanceApplications: X'mas dec.. |
|||
Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America E 8701A Short Glass Fiber Reinforced Epoxy E 8701A is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability and good strength at elevated temperatures.Information provided by Sumitomo Bak North Amer.. |
|||
Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | ASTM D256 |
Styrolution NAS® 36 UV Stabilized Acrylic Copolymer Features:Sparkling clarity Excellent indoor light stability Styrenic processing advantages Scratch resistant Enhanced mold releaseApplications:Appliances Point-of -Purchase Displays Toys Office Acce.. |
|||
Izod Impact, Notched | 0.200 J/cm @Thickness 3.20 mm |
0.375 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SC 203EL General Purpose Polystyrene CharacteristicsMedium flow grade with good mechanical properties Improves productivity due to good balance of flow, heat and mold release propertiesProcessing Injection moldingApplicationsAudio cass.. |
|||
Izod Impact, Notched | 0.200 J/cm @Temperature -30.0 °C |
0.375 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL FXN4020H PPE+HIPS high gloss Noryl |
|||
Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | ASTM D256 |
Goodfellow TPX® RT31XB Injection Molding Grade Polymethylpentene This grade is highly recommended for injection molding; also for film and fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release c.. |
|||
Izod Impact, Notched | 0.200 J/cm @Temperature 23.0 °C |
0.375 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTASTIR GP 1000 Polystyrene Polystyrene crystal, general purposeGood melt flow rate, stiffness, gloss, excellent transparencyInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | UV Postcure; ASTM D256A |
DSM Somos® BioClear Parts created with Somos® BioClear are designed for medical applications that are non-implant and have limited contact with the body such as device prototyping. They are shatter-resistant so they w.. |
|||
Izod Impact, Notched | 0.200 J/cm @Temperature >=23.0 °C |
0.375 ft-lb/in @Temperature >=73.4 °F |
ASTM D256 |
Carmel Olefins CAPILENE® W 77 AV Polypropylene Homopolymer CAPILENE® W 77 AV is a very high melt flow rate polypropylene homopolymer for injection molding with antistatic and nucleating additives. It offers a good balance of stiffness and flow, high de-mol.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATS 134 Phenolic Molding Inorganic, graphite Filler, Compression Molded Characteristics: Low coefficient of frictionSelf lubricating ( graphite modified )Good thermal conductivityGood glide propertiesNot suitable for electrical applicationColor- black gray Soft/medium f.. |
|||
Izod Impact, Notched | 0.200 J/cm @Diameter 3.17 mm |
0.375 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 1220 High Heat Crystal Polystyrene
(discontinued **) Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |
|||
Izod Impact, Notched | 0.200 J/cm @Diameter 3.17 mm |
0.375 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 3510 General Purpose Crystal Polystyrene
(discontinued **) Excellent blending resin, Suitable fore difficult to fill and thin wall molding, USP Class VIApplications: Single service cutlery, Cosmetic and medical molding, Consumer electronic packagingExposure.. |
|||
Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | ASTM D256 |
Ineos Nova 8048 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Improved toughness, Custom colorsApplications: Designed for injection molding applications requiring clarity and toughnessPerformance grades of polystyrene are engineered to have specific properties.. |
|||
Izod Impact, Notched | 0.200 - 2.45 J/cm | 0.375 - 4.59 ft-lb/in | Average value: 0.585 J/cm Grade Count:94 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched | 0.200 - 0.500 J/cm @Temperature -18.0 - -18.0 °C |
0.375 - 0.937 ft-lb/in @Temperature -0.400 - -0.400 °F |
Average value: 0.275 J/cm Grade Count:4 |
Overview of materials for Acrylic, Optical Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H08U-00 Polypropylene Homopolymer, Fiber Grade Suggested fabrication methods: Fiber spinningFeatures: UV stable, High tenacityTypical applications: Geotextiles, Continuous filamentComplies with FDA specification, Title 21, CFR 177.1520.Typical p.. |
|||
Izod Impact, Notched | 0.200 J/cm @Diameter 3.17 mm |
0.375 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ISO 180 |
Ineos Nova 610 Crystal Polystyrene GP Grade
(discontinued **) Broad, medium melt flow range, Broad Vicat rangeApplications: Any; Injection Molding and ExtrusionProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise spe.. |
|||
Izod Impact, Notched | 0.200 J/cm @Diameter 3.17 mm |
0.375 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ISO 180 |
Ineos Nova 207 Crystal Polystyrene High Heat, High Flow Grade
(discontinued **) Fast cycling, Excellent flow characteristics, Extrusion and Injection Molding Applications: XPS sheet, Foam insulation, CD and DVD jewel boxesProperties were determined on injection molded specimen.. |
|||
Izod Impact, Notched | 0.200 - 5340 J/cm | 0.375 - 10000 ft-lb/in | Average value: 1.44 J/cm Grade Count:54 |
Overview of materials for Polypropylene, Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Blow Molding Grade". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar |
Ineos H13Z-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical prope.. |