Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.120 J/cm | 0.225 ft-lb/in | ASTM D256 |
SABIC PS 126 General Purpose Polystyrene for Injection Molding Product Description: General purpose Polystyrene PS 125 is manufactured by continuous mass polymerization of styrene monomer. It is a crystal-like, hard and brittle polymer with medium flow and hi.. |
|||
Izod Impact, Notched | 0.120 - 0.220 J/cm | 0.225 - 0.412 ft-lb/in | ASTM D256 |
Proto3000 Accura® 55 Plastic Stereolithography (SLA) Prototyping Polymer Simulate the look and feel of molded ABS with this tough and versatile plastic.Features:Durable and rigid materialLook and feel of molded ABSHigh accuracy with less distortionHigh production speedLo.. |
|||
Izod Impact, Notched | 0.120 J/cm @Temperature -30.0 °C |
0.225 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycolac® INP581 ABS+SAN High flow, low molecular weight SAN. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for.. |
|||
Izod Impact, Notched | 0.120 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.225 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
IRPC Polimaxx Polene HI830 Polystyrene APPLICATIONS: EXTRUSION APPLICATION, VACUUM SHEET : FOOD PACKAGING ELECTRICAL APPLIANCES, HOUSEHOLD PRODUCT, TOYS, SANITARY, etc. |
|||
Izod Impact, Notched | 0.120 - 0.150 J/cm | 0.225 - 0.281 ft-lb/in | ASTM D256A |
DSM Somos® NanoTool™ Resin for Stereolithography, UV Postcure DescriptionNanoTool produces strong, stiff, high temperature resistant composite parts on conventional stereolithography machines. This third generation of Somos® ProtoComposite materials is heavi.. |
|||
Izod Impact, Notched | 0.120 - 0.220 J/cm | 0.225 - 0.412 ft-lb/in | ASTM D256 |
3D Systems Accura® 55 Plastic for SLA® Systems Simulate the properties and appearance of molded ABS. For use with solid-state stereolithography (SLA®) systems.ApplicationsAutomotive interior componentsShort-run production partsElectronic compon.. |
|||
Izod Impact, Notched | 0.120 J/cm | 0.225 ft-lb/in | ASTM D256 |
SABIC PS 100 General Purpose Polystyrene for Injection Molding Product Description: General purpose Polystyrene PS 100 is manufactured by continuous mass polymerization of styrene monomer. It is a crystal-like, hard and brittle polymer with good flow properti.. |