Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPC T4020 E20 Polypropylene Copolymer, Mineral Reinforced, Modified Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL A63 E Raw extruded nylon 6.6 for injection molding Raw extruded nylon 6.6 for injection molding (available only in nature).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 HS-GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced Nylon 6.6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 241R PC (Europe-Africa-Middle East) LEXAN 241R is a medium viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.8 mm approved. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 241RX PC (Europe-Africa-Middle East) LEXAN 241RX is a medium viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.75 mm and allows for the molder to use up to 50 percent regri.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 955 PC (Europe-Africa-Middle East) Lexan* 955 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque color.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 955AU PC (Europe-Africa-Middle East) Lexan* 955AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXD921A PC (Europe-Africa-Middle East) LEXAN FXD921A is a transparent/translucent, medium viscosity, flame retardent grade for light diffusion special effects. Color package may affect performance. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer (Europe-Africa-Middle East) 18 MFR LEXAN High Flow Ductile Copolymer |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® IFX3420Z PC (Asia Pacific) Lexan* IFX3420Z is a medium viscosity, release containing, injection moldable, polycarbonate grade suitable for use in industry protective eye-ware welding applications. This grades meets the transm.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® IFX5420Z PC (Asia Pacific) Lexan* IFX5420Z is a medium viscosity, release containing, injection moldable polycarbonate grade suitable for use in industry protective eye-ware welding applications. This grade meets the transmis.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® OQ3732 PC (Europe-Africa-Middle East) High Viscosity, UV-stabilized PC for ophthalmic lenses. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycolac® DL100 ABS (Europe-Africa-Middle East) CYCOLAC DL100 is a high heat, high impact, low emissions ABS/PC blend. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 141R PC (Europe-Africa-Middle East) LEXAN 141R is a medium viscosity multi purpose grade and contains a release agent to ensure easy processing. LEXAN 141R is available in transparent, translucent and opaque colours. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | ISO 179/1eA |
Pasargad Polymer Peyvand Pasamid 3P-H1150B Nylon 6, 50% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Grupo Repol Dinalon® B1S25 MI PA6 Medium Impact Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 218 V35 Black 21NHFE PA66, 35% glass fiber, Conditioned Description: TECHNYL® A 218 V35 BLACK 21NHFE is polyamide 6.6, high flow, reinforced with 35% glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefit.. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | ISO 179 |
Styrolution Terblend® N NG-06 30% Glass Filled ABS/PA6 (Dry) Terblend N NG-06 is a 30% glass fiber reinforced ABS/PA6 blend with extra high rigidity and dimensional stability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® IQ420HP PBT Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 MZ 301 CP Combination Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 CF10 HWCP 10% Carbon Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Stanyl® TW241F10 (DAM) Nylon 46 50% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® TSG-50/4 W PA666-GF50 Product description: Grilon TSG-50/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Akro-Plastic Akromid® B3 GF 20 (2470) PA 6 Conditioned, 20% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | ISO 179/1eA |
CENTROPLAST CENTROTRON GF 15 Polyphenylene sulfide 15% glass fiber CENTROTRON is a plastic that is resistant to oxidation and hydrolysis which can be used in high temperature applications. CENTROTRON has a low sliding friction coefficient and high abrasion resista.. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | ISO 179/1eA |
BASF Ultramid® A3EG7 35% Glass Filled PA66 (Dry) Ultramid A3EG6 is a 35% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 73G30TGI BK267 Nylon 6
(Unverified Data**) Zytel® 73G30TGI BK267 is a 30% glass fiber reinforced, toughened, black polyamide 6 optimized for gas injection molding process.Information provided by DuPont Performance Polymers |