Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.940 J/cm² - NB
4.47 ft-lb/in² - NB
Average value: 6.67 J/cm² Grade Count:65
Overview of materials for Polyester Thermoplastic Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values..
Charpy Impact, Notched 0.940 - 0.990 J/cm²

@Temperature -30.0 - -30.0 °C
4.47 - 4.71 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.965 J/cm² Grade Count:2
Overview of materials for Nylon 11 with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are includ..
Charpy Impact, Notched 0.940 J/cm²

@Temperature -30.0 °C
4.47 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® BZM 23 G9 Nylon 11, 23% Glass Fiber Filled (Dry)
Designation ISO 1874-PA11,MS,18-040,(G+C)(F+D)(25+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Additive free.Rigidity. Low fric..
Charpy Impact, Notched 0.940 J/cm²

@Temperature -30.0 °C
4.47 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® ASR 30 Nylon 12, 30% Carbon Fiber Filled (Dry)
Designation ISO 1874-PA12,M,16-120,CF30Rigid grade with carbon fiber filler (30%) for injection molding. Available color: black.Very high rigidity. High strength-to-weight ratio. Very low shrinkage:..