Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 8.20 J/cm² | 39.0 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and up to 25% post consumer recycle content. Availability of resin is restricted and lead times are.. |
|||
Charpy Impact, Notched | 8.20 J/cm² | 39.0 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer (Asia Pacific) 7 MFR LEXAN HFD Copolymer |
|||
Charpy Impact, Notched | 8.20 J/cm² | 39.0 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer (Europe-Africa-Middle East) 7 MFR LEXAN HFD Copolymer |
|||
Charpy Impact, Notched | 8.20 J/cm² | 39.0 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer 7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only |
|||
Charpy Impact, Notched | 8.20 J/cm² | 39.0 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer (Asia Pacific) 7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only |
|||
Charpy Impact, Notched | 8.20 J/cm² | 39.0 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer (Europe-Africa-Middle East) 7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only |
|||
Charpy Impact, Notched | 8.20 J/cm² | 39.0 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® HPS4 PC Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).EtO, steam, e-beam, and gamma sterilizable... |
|||
Charpy Impact, Notched | 8.20 J/cm² | 39.0 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® HPS4 PC (Asia Pacific) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).EtO, steam, e-beam, and gamma sterilizable... |
|||
Charpy Impact, Notched | 8.20 J/cm² | 39.0 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® HPS4 PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).EtO, steam, e-beam, and gamma sterilizable... |
|||
Charpy Impact, Notched | 8.20 J/cm² | 39.0 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer (Asia Pacific) Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 25% post consumer recycle content. Limited availability and restricted color only. Higher color.. |
|||
Charpy Impact, Notched | 8.20 J/cm² | 39.0 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer 7 MFR LEXAN HFD Copolymer |
|||
Charpy Impact, Notched | 8.20 J/cm² | 39.0 ft-lb/in² | ISO 179 |
Menzolit Menzolit® SMC 0390 Unsaturated Polyester UP SMC 0390 is a standard low profile SMC. Because of its low shrinkage, the material shows good surface quality as well as very low warpage. The product is suitable for applications if a better surfac.. |
|||
Charpy Impact, Notched | 8.20 J/cm² | 39.0 ft-lb/in² | |
Arkema Group Orgalloy® LT 4060IH Flexible Nylon Alloy (Conditioned) Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrate a good balance of properties eg, high flexibility (200 MPa), good .. |