Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS (Asia Pacific) PC+ ABS Automotive applications |
|||
Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS (Europe-Africa-Middle East) PC+ ABS automotive applications, excellent flow/impact balance, high heat resistance temperature and excellent properties retention after hydrolytic and heat aging. |
|||
Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 920 PC (Europe-Africa-Middle East) LEXAN 920 is a low viscosity flame retardant grade, especially suitable for electrical applications. |
|||
Charpy Impact, Notched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1434T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me.. |
|||
Charpy Impact, Notched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb.. |
|||
Charpy Impact, Notched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb.. |
|||
Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HF1110R PC (Europe-Africa-Middle East) LEXAN HF1110R is a high flow grade especially designed for applications that require thin wall sections and high flow lengths. |
|||
Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® LSHF PC (Asia Pacific) Clear PolyCarbonate, High Flow, UV Stabilization, Heat Stabilization |
|||
Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® LSHF PC (Europe-Africa-Middle East) Clear PolyCarbonate, High Flow, UV Stabilization, Heat Stabilization |
|||
Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® ML3400 PC (Europe-Africa-Middle East) LEXAN ML3400 is a medium viscosity, impact modified grade with improved chemical resistance. It passes the British Standard 2495 and 5361 solvent tests. |
|||
Charpy Impact, Notched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® ML7647 PC Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque onlyThis data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® ML7647K PC (Asia Pacific) Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque only |
|||
Charpy Impact, Notched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Charpy Impact, Notched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL9414T PC Copolymer (Asia Pacific) Lexan* EXL9414T resin grade is a halogen-free flame retardant polycarbonate featuring transparency, -40 degree C ductility and UL-94 V0 rating for injection molding applications. Excellent impact co.. |
|||
Charpy Impact, Notched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer (Asia Pacific) Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af.. |
|||
Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer (Europe-Africa-Middle East) 55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only |
|||
Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Europe-Africa-Middle East) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Charpy Impact, Notched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics LNP Thermocomp ML4351HF PC (Asia Pacific) LNP* Thermocomp* ML4351HF is a Light Reflecting Grade.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Charpy Impact, Notched | 6.00 - 12.0 J/cm² | 28.6 - 57.1 ft-lb/in² | DIN 53453 |
Zell-Metall Engineering Plastics Zellamid 1115 at 50% RH By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads .. |
|||
Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | IS0179-1:2000 |
Zhejiang Juner PC-A2-1 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | IS0179-1:2000 |
Zhejiang Juner PC-A2-9 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | IS0179-1:2000 |
Zhejiang Juner PC-A7 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | ISO 179/1eA |
Covestro Makroblend® DP UT6000 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedinjection molding grade Makroblend DP UT6000* offers an exceptional low-temperature impact strength, good flowability and excellent chemical resis.. |
|||
Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | ISO 179/1eA |
Covestro Makroblend® KU 2-7912 MBS151 Polycarbonate + PBT, Impact Grade (PC+PBT)-blendsimpact modifiedInjection molding grademedium flowhigh toughness at low temperaturesideal for painted applicationunreinforcedAs of 1 September 2015, Bayer MaterialScience was separated.. |
|||
Charpy Impact, Notched | 6.00 J/cm² @Temperature 30.0 °C |
28.6 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4158 nat PA612 Product description: Grilamid XE 4158 natural is a medium viscosity Polyamide 12 with super high impact strength. The main features of Grilamid XE 4158 natural are: Very good hydrolysis resistanceGo.. |
|||
Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® TR 90 NZZ nat PAMACM12-I Product description: Grilamid TR 90 NZZ natural is an amorphousthermoplastic polyamide, based on aliphatic and cycloaliphatic units. Grilamid TR 90 NZZ natural offers a variety of interesting proper.. |
|||
Charpy Impact, Notched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultramid® B3K BK00464 PA6 (Conditioned) Description: Easy flowing and stabilized injection-molding grade used for technical parts with wall thicknesses >2 mm, e.g. machinery components, fans and power tool housings.Information provided by.. |
|||
Charpy Impact, Notched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL9414T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL9414T resin grade is a halogen-free flame retardant polycarbonate featuring transparency, -40 degree C ductility and UL-94 V0 rating for injection molding applications. Excellent impact co.. |