Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.590 J/cm² @Temperature -30.0 °C |
2.81 ft-lb/in² @Temperature -22.0 °F |
|
Eastman Eastar DN007 PCTG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Charpy Impact, Notched | 0.590 J/cm² @Temperature -30.0 °C |
2.81 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Lustran® Elite HH 1891 Key Features:UnfilledHeat stabilized or stable to heatSuitable processing methods:Injection molding |
|||
Charpy Impact, Notched | 0.590 J/cm² @Temperature -30.0 °C |
2.81 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® AECN TL Nylon 12, Cable Sheathing Grade (Conditioned) Designation ISO 1874-PA12,KHL,14-010Extrusion grade for the sheathing of wires and cables. Available colors: natural and orange. Heat and light stabilized.Low melt viscosity. High speed extrusion. V.. |
|||
Charpy Impact, Notched | 0.590 J/cm² @Temperature -30.0 °C |
2.81 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® ARVO 950 TLD Nylon 12, Rotomolding Grade (Conditioned) Designation ISO 1874-PA12,RHLR,16-010Grade for rotomolding. Available color: natural. Light and heat stabilized. Mold-release agent.Easy to be processed in the same conditions as polyethylene. High .. |
|||
Charpy Impact, Notched | 0.590 J/cm² | 2.81 ft-lb/in² | 1eA; ISO 179 |
Azoty Tarnow™ TARNOFORM 300 GF5 POM 26% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Charpy Impact, Notched | 0.590 J/cm² @Temperature -30.0 °C |
2.81 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® AMN D Nylon 12, Rigid, Injection Grade (Conditioned) Designation ISO 1874-PA12,MR,14-010Rigid grade for injection molding. Available colors: black, natural, orange, red and white. Possibilities of heat and light stabilizing agents. Mold-release agent... |
|||
Charpy Impact, Notched | 0.590 J/cm² @Temperature 23.0 °C |
2.81 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultramid® B35G3 BK 00564 15% Glass Filled PA6 (Dry) Description: 15% glass fiber reinforced injection molding grade e.g. for internal gas pressure applications such as flashing direction switch gears, automobile mirror housings and wheels of mountain.. |
|||
Charpy Impact, Notched | 0.590 J/cm² | 2.81 ft-lb/in² | ISO 179 |
BASF Ultradur B 4040 G4 LS High Speed BK15029 20% Glass Filled PBT/PET |
|||
Charpy Impact, Notched | 0.590 J/cm² | 2.81 ft-lb/in² | ISO 179/1eA |
Polyplastics Duracon® NW-02 Acetal Co-polymer (POM), High sliding, Special lubricant, High sliding DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Charpy Impact, Notched | 0.590 J/cm² @Temperature -30.0 °C |
2.81 ft-lb/in² @Temperature -22.0 °F |
|
Eastman Tenite 105-23 Cellulose Acetate
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |