Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | >= 2.50 J/cm² | >= 11.9 ft-lb/in² | ISO 179 |
Murtfeldt Muralen® Black Antistatic Polyethylene, Conductive Muralen® is based on high molecular weight polyethylene (PE-HMW) and is ideally suited for use in applications that require the generally impressive material properties of polyethylene. Because of.. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | ISO179/3C DIN.53453 |
Omnia Plastica Omniamid PA 6 - Akulon 6 - at 50% RH Semi-crystalline polymer of polyamide obtained by the polymerisation of the caprolactam. Its large popularity is due to both its good overall features as well as its cost-performance relationship. T.. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS (Asia Pacific) PC+ABS, ECO-conforming flame retardant with metallic or pearlescent appearance. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 244R PC 10.5 MFR. Improved flame retardance. USA FDA compliant (limited colors). Internal mold release. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® 923 PC (Europe-Africa-Middle East) LEXAN 923 is a low viscosity flame retardant, UV-stabilized grade, especially suitable for electrical applications. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer (Asia Pacific) 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Asia Pacific) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® FXC810SK PC+ABS Color package may affect performance. Visual Fx PC+ABS in various metallic (sparkle) colors. High heat/good flow characteristics. Appliance/automotive/telecommunication uses. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL PX6120 PPE+PS (Asia Pacific) Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
80*10*4mm, Cut; ISO 179/1eA |
SABIC Innovative Plastics SABIC STAMAX 30YM243 PP SABIC® STAMAX 30YM243 is a 30% long glass fiber reinforced UV stabilized polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMD.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Europe-Africa-Middle East) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -20.0 °C |
11.9 ft-lb/in² @Temperature -4.00 °F |
ISO 179/2C |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Europe-Africa-Middle East) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Styron CALIBREâ„¢ MEGARAD 2081-15 Polycarbonate Resin Overview: CALIBREâ„¢ MEGARAD 2081-15 Polycarbonate resin provides end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to hi.. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | |
Sibur Discar-E PC/ABS Compositional Polymer Composition material PC/ABS with high shock resistance, thermal, light, and atmospheric resistance for profile articles of technical purpose and for sheets with following pneumatic formation of auto.. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | |
Sibur Discar-L PC/ABS Compositional Polymer Composition material PC/ABS with high shock resistance, thermal, light, and atmospheric resistance for structural parts of technical purpose and parts for internal finishing of automobiles. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | |
Sibur Discar-SL PC/ABS Compositional Polymer Composition material PC/ABS with low viscosity of melting with high shock resistance, thermal and atmospheric resistance for large, thin wall structural parts of automobile interiors. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Covestro Makroblend® DP UT3907 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendhigh flowimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT3907* offers superior flowability, good impact strength and excellent ch.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 30.0 °C |
11.9 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® ELX 40 HNZ TPA Product description: Grilon ELX 40 H NZ is a high viscosity, heat stabilized, impact modified, thermoplastic PA6 elastomer for extrusion blow moulding applications. Grilon ELX 40 H NZ has the follow.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600/50 GV 15 HWCP 15% Glass Fiber Nylon 66, Impact Modified Until 0°C, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® LVX-50H black 9230 PA12-GF50 Product description: Grilamid LVX-50H black 9230 is a 50% glass fiber reinforced, heat stabilized polyamide 12. Special characteristics of this injection molding product are: Very high stiffness and.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 30.0 °C |
11.9 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® R 50 H NZ PA6 Product description: Grilon R 50 H NZ is a high viscosity, unreinforced, heat stabilized, impact modified PA6 extrusion blow molding grade. Grilon R 50 H NZ has the following important properties: V.. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® TSGL-40/4 black 9833 PA666-GF40 Product description: Grilon TSGL-40/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 black is characterized by the following key-p.. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Delrin® 100T NC010 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer Delrin 100T NC010 is a toughened high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | ISO 179 |
Chi Mei Polylac® PA-746 ABS - High Flow High flow, medium impact |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**) 30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T BK261 is a 30% glass fiber reinforced toughened black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polym.. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® FG408L NC010 Nylon 66
(Unverified Data**) Unreinforced Toughened Polyamide 66 with Developed for Food Contact Applications Zytel FG408L NC010 is a general purpose lubricated impact modified polyamide 66 resin with superior toughness for inj.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Conditioned) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | Conditioned; ISO 179/IeA |
Addiplast Addinyl PMD 20090 Nylon 6, 40% Glass Filled Glass fiber reinforced, high resistance to frictionInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® BG-50 FC PA6-GF50 Product description: Grilon BG-50 FC is a heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 FC has the following important properties: Short cycle timesExcellent surfac.. |