Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | ISO 179-1/1eA |
Quadrant EPP Ertalyte® TX PET + solid lubricant, extruded (ISO Data) Ertalyte TX is a polyethylene terephthalate compound incorporating a uniformly dispersed solid lubricant. Its specific formulation makes it a premium internally lubricated bearing-grade. Ertalyte TX.. |
|||
Charpy Impact, Notched | 0.250 - 0.350 J/cm² @Temperature 23.0 °C |
1.19 - 1.67 ft-lb/in² @Temperature 73.4 °F |
Injection and Compression; ISO 179/ 1eA |
Raschig Group 3505 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Charpy Impact, Notched | 0.250 - 0.450 J/cm² | 1.19 - 2.14 ft-lb/in² | Compression; ISO 179/1eA |
Raschig Group 6551 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Charpy Impact, Notched | 0.250 - 0.400 J/cm² @Temperature 23.0 °C |
1.19 - 1.90 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eA |
Raschig Group 6552 DAIP Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Charpy Impact, Notched | 0.250 - 2.50 J/cm² @Temperature -30.0 - -20.0 °C |
1.19 - 11.9 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.841 J/cm² Grade Count:49 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL A63 AV15 Nylon 6.6 for injection molding Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | ISO 179-1/1eA |
Quadrant EPP Duratron® PBI CU60 compression moulded (ISO Data) Duratron CU60 PBI is very “clean” in terms of ionic impurity and does not outgas (except water). These characteristics make this material extremely attractive to high-tech industries such as semic.. |
|||
Charpy Impact, Notched | 0.250 - 1.10 J/cm² | 1.19 - 5.24 ft-lb/in² | Average value: 0.582 J/cm² Grade Count:4 |
Overview of materials for PVC, Rigid Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Charpy Impact, Notched | 0.250 - 1.24 J/cm² @Temperature -30.0 - -30.0 °C |
1.19 - 5.90 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.640 J/cm² Grade Count:24 |
Overview of materials for Nylon 12, Extrusion/Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values .. |
|||
Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | ISO 179 |
Manifattura Cattaneo PET+PTFE Polyethylene Terephthalate Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -23.0 °C |
1.19 ft-lb/in² @Temperature -9.40 °F |
DIN 53453 |
Global PP-1111-R Polypropylene Homopolymer Description-transparency, high stiffness, high heat resistantApplications-electrical/electronic Information provided by Global Polymers Corporation. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
Global PP-2300-SC Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-thin walled parts, electrical appliancesInformation provided by Global Polymers Corporation. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
|
LATI Latene® 11 MDT05-01 PP Homopolymer Polypropylene homopolymer (PPh) based compound. Magnetic detectable filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industr.. |
|||
Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | |
LATI Latigray 53/22-01 CX/70 PP Homopolymer, Impact Modified Radiopaque compound based on Polypropylene homopolymer (PPh), impact modified. Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Daplen™ MD206U Polypropylene Compound 20% Mineral Filled Daplen MD206U is a 20% mineral filled polypropylene compound intended for injection molding. MD206U has been developed especially for automotive interior parts that require excellent balance betwee.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis HG313MO Polypropylene HG313MO is a polypropylene homopolymer intended for injection molding. Its high melt flow makes it especially suitable for products with long flow length. This grad is designed for high-speed inject.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis HH315MO Polypropylene HH315MO is a polypropylene homopolymer intended for injection molding. Its high melt flow makes it especially suitable for products with long flow length. This grade is designed for high-speed injec.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Unipetrol PP MONSTEN® MA 230 Polypropylene Homopolymer Applications include injection molding. Antistatic stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Unipetrol PP MONSTEN® MA 350 Polypropylene Homopolymer Applications include injection molding. Antistatic stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -30.0 °C |
1.19 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Borealis Daplen™ AK4504 TPO Compound Daplen AK4504 is a 30% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen AK4504 is a material with excellent impact/stiffness ratio. Thanks to its low th.. |
|||
Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | ISO 179/1eA |
Borealis Xmod™ HF006SA High Stiffness Polypropylene for Injection Molding Applications Xmod HF006SA is a high melt flow PP homopolymer with increased crystallinity, intended for injection molding. Xmod HF006SA is specifically developed for applications demanding a high surface appear.. |
|||
Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | ISO 179 |
Vyncolit 4421 XB Novolac Phenolic Mineral and organic filled phenolic molding compound with good mechanical properties.USES: Fuse holders, brush holders, circuit breakers, automotive ignition and solenoid covers.Information provided.. |
|||
Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | ISO 179/IeA |
Addiplast Addilene H 652 Polypropylene Homopolymer High temperature resistance, high gloss, very good surface appearanceInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | ISO 179-1eA |
Barlog Plastics KEBAFORM C 906 GB POM Copolymer, 30% glass bead reinforced POM-GB30Information provided by BARLOG plastics GmbH. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -30.0 °C |
1.19 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 2348 M Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | ISO 179/1eA |
CENTROPLAST CENTROLYTE ZX Polyethylene terephthalate with lubricant This material's solid lubricant additive has good sliding properties, and is well suited for high load, dry running situations. Possible uses include precision plain bearings, plug connectors, r.. |
|||
Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | ISO 179-1/1eA |
Murtfeldt Murylat® SP Polyethylene Terephthalate Murylat® SP combines the properties of Murylat® with improved wear and friction characteristics. It also has increased dynamic resilience which, for example, significantly reduces the required dri.. |
|||
Charpy Impact, Notched | 0.250 - 1.10 J/cm² @Temperature -30.0 - -30.0 °C |
1.19 - 5.24 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.629 J/cm² Grade Count:7 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Charpy Impact, Notched | 0.249 J/cm² | 1.19 ft-lb/in² | ASTM D256 |
Plenco 7579 Phenolic, Granular, Compression Molded PLENCO 07579 is a fast curing, woodflour filled, novolac phenolic molding compound, formulated for industrial applications that do not require a smooth finish. UL recognized under component file E40.. |