Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.170 - 2.00 J/cm² | 0.809 - 9.52 ft-lb/in² | Average value: 0.756 J/cm² Grade Count:123 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Charpy Impact, Notched | 0.170 J/cm² @Temperature -30.0 °C |
0.809 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Centrex® 815 ASA Blend
(discontinued **) Key Features:UnfilledLight stabilized or stable to lightU.V. stabilized or stable to weatherHeat stabilized or stable to heatSuitable processing methods:Injection moldingInformation provided by Baye.. |
|||
Charpy Impact, Notched | 0.170 - 0.210 J/cm² | 0.809 - 0.999 ft-lb/in² | Average value: 0.188 J/cm² Grade Count:4 |
Overview of materials for Phenolic, Novolac, Heat Resistant Grade, Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Heat Resistant Grade, Filled". Each property range of values reported is minimum and .. |
|||
Charpy Impact, Notched | 0.170 J/cm² | 0.809 ft-lb/in² | ASTM D256 |
Plenco 4100 Phenolic, Granular, Injection Molded
(discontinued **) Two-stage Phenolic. PLENCO 04100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability characteristics and molded finish. It is used in appliance and .. |
|||
Charpy Impact, Notched | 0.170 J/cm² | 0.809 ft-lb/in² | ASTM D256 |
Plenco 4246 Phenolic, Granular, Injection Molded
(discontinued **) Two-stage Phenolic. PLENCO 04246 flow 18 is a black two-stage, medium heat resistant phenolic molding compound. It has excellent electrical, moldability and molded finish characteristics. It is use.. |
|||
Charpy Impact, Notched | 0.170 J/cm² | 0.809 ft-lb/in² | J/cm; ASTM D256 |
Plenco Valite 1246-18X Novolac Phenolic, Granular, Injection Molded
(discontinued **) This Valite product has been replaced by Plenco 4246. Data provided by Plenco.VALITE 1246-18X is a black two-stage, medium heat resistant phenolic molding compound. It has excellent electrical, mol.. |
|||
Charpy Impact, Notched | 0.170 J/cm² | 0.809 ft-lb/in² | J/cm; ASTM D256 |
Plenco Valite 4100 Novolac Phenolic, Granular, Injection Molded
(discontinued **) This Valite product has been replaced by Plenco 4100. Data provided by Plenco.VALITE 4100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability charac.. |
|||
Charpy Impact, Notched | 0.170 J/cm² | 0.809 ft-lb/in² | ISO 179/1eA |
Lucite International Diakon® Frost 902 51 Acrylic Polymer Information provided by Lucite International |
|||
Charpy Impact, Notched | 0.170 J/cm² @Temperature 23.0 °C |
0.809 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Topas Advanced Polymers TOPAS® 6013M-07 Cyclic Olefin Copolymer (COC) TOPAS® 6013M-07 is an injection molding grade with a wide processing window, especially suited for blow molding processes including IBM and ISBM. It is a glass-clear amorphous polymer with outstand.. |
|||
Charpy Impact, Notched | 0.170 J/cm² @Temperature -30.0 °C |
0.809 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1184 L Polypropylene Nucleated grade with high processing stability containing antistatic for thermoformed parts.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.170 J/cm² @Temperature -30.0 °C |
0.809 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1102 K Polypropylene Grade with high processing stability for film tape (low water carryover), fibrillated film, monofilaments, OPP film (special formulations) and thermoformed parts.Data was collected by ISO methods an.. |
|||
Charpy Impact, Notched | 0.170 J/cm² @Temperature -30.0 °C |
0.809 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1104 K Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.170 - 1.00 J/cm² | 0.809 - 4.76 ft-lb/in² | Average value: 0.442 J/cm² Grade Count:17 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |