Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.160 - 7.50 J/cm² | 0.761 - 35.7 ft-lb/in² | Average value: 1.35 J/cm² Grade Count:19 |
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an.. |
|||
Charpy Impact, Notched | 0.210 - 7.50 J/cm² | 0.999 - 35.7 ft-lb/in² | Average value: 0.984 J/cm² Grade Count:155 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Charpy Impact, Notched | 0.400 - 7.50 J/cm² | 1.90 - 35.7 ft-lb/in² | Average value: 4.77 J/cm² Grade Count:111 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Charpy Impact, Notched | 0.300 - 7.50 J/cm² | 1.43 - 35.7 ft-lb/in² | Average value: 2.89 J/cm² Grade Count:5 |
Overview of materials for Polypropylene, Mineral Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced, Impact Modified". Each property range of values reported is minimum a.. |
|||
Charpy Impact, Notched | 0.200 - 7.50 J/cm² | 0.952 - 35.7 ft-lb/in² | Average value: 1.07 J/cm² Grade Count:127 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Charpy Impact, Notched | 0.300 - 7.50 J/cm² | 1.43 - 35.7 ft-lb/in² | Average value: 2.15 J/cm² Grade Count:27 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |