Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.300 - 1.60 J/cm² @Temperature -40.0 - 30.0 °C |
1.43 - 7.61 ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 0.901 J/cm² Grade Count:89 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Charpy Impact, Notched | 0.200 - 1.60 J/cm² | 0.952 - 7.61 ft-lb/in² | Average value: 0.396 J/cm² Grade Count:23 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Charpy Impact, Notched | 1.40 - 1.60 J/cm² @Temperature -30.0 - -30.0 °C |
6.66 - 7.61 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.50 J/cm² Grade Count:4 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Charpy Impact, Notched | 1.40 - 1.60 J/cm² @Thickness 3.00 - 3.00 mm |
6.66 - 7.61 ft-lb/in² @Thickness 0.118 - 0.118 in |
Average value: 1.50 J/cm² Grade Count:4 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Charpy Impact, Notched | 1.40 - 1.60 J/cm² @Temperature -30.0 - -30.0 °C |
6.66 - 7.61 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.55 J/cm² Grade Count:4 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact, Notched | 1.40 - 1.60 J/cm² @Thickness 3.00 - 3.00 mm |
6.66 - 7.61 ft-lb/in² @Thickness 0.118 - 0.118 in |
Average value: 1.55 J/cm² Grade Count:4 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact, Notched | 1.20 - 1.60 J/cm² @Temperature -30.0 - -30.0 °C |
5.71 - 7.61 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.62 J/cm² Grade Count:4 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Charpy Impact, Notched | 1.20 - 1.60 J/cm² @Thickness 3.00 - 3.00 mm |
5.71 - 7.61 ft-lb/in² @Thickness 0.118 - 0.118 in |
Average value: 1.62 J/cm² Grade Count:4 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Charpy Impact, Notched | 1.40 - 1.60 J/cm² @Temperature -30.0 - -30.0 °C |
6.66 - 7.61 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.44 J/cm² Grade Count:16 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Charpy Impact, Notched | 1.40 - 1.60 J/cm² @Thickness 3.00 - 3.00 mm |
6.66 - 7.61 ft-lb/in² @Thickness 0.118 - 0.118 in |
Average value: 1.44 J/cm² Grade Count:16 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Charpy Impact, Notched | 0.110 - 1.60 J/cm² @Temperature -30.0 - -30.0 °C |
0.524 - 7.61 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.507 J/cm² Grade Count:20 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Charpy Impact, Notched | 0.200 - 1.60 J/cm² | 0.952 - 7.61 ft-lb/in² | Average value: 0.682 J/cm² Grade Count:83 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact, Notched | 0.600 - 1.60 J/cm² | 2.86 - 7.61 ft-lb/in² | Average value: 0.872 J/cm² Grade Count:8 |
Overview of materials for Nylon 66, 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in.. |
|||
Charpy Impact, Notched | 0.200 - 1.60 J/cm² | 0.952 - 7.61 ft-lb/in² | Average value: 0.569 J/cm² Grade Count:28 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact, Notched | 0.800 - 1.60 J/cm² @Temperature -30.0 - 0.000 °C |
3.81 - 7.61 ft-lb/in² @Temperature -22.0 - 32.0 °F |
Average value: 1.23 J/cm² Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
Charpy Impact, Notched | 0.300 - 1.60 J/cm² @Temperature -30.0 - -30.0 °C |
1.43 - 7.61 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.789 J/cm² Grade Count:60 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |
|||
Charpy Impact, Notched | 0.850 - 1.60 J/cm² | 4.05 - 7.61 ft-lb/in² | Average value: 1.06 J/cm² Grade Count:14 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |