Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 2.90 J/cm² | 13.8 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycolac® MG38 ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Charpy Impact, Notched | 2.90 J/cm² | 13.8 ft-lb/in² | |
Polimeri Europa SINKRAL B620 ABS, Impact Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-04-25-20 High impact injection moulding grade. Its` excellent balance of mechanical properties (toughness -.. |
|||
Charpy Impact, Notched | 2.90 J/cm² | 13.8 ft-lb/in² | ISO 179 |
GEHR Plastics PE-HD Polyethylene HDPE Polyethylene has a good chemical resistance against almost all acids and bases, detergents and hot water. PE has good insulation properties and is easy to weld. The operating temperature is from -50.. |
|||
Charpy Impact, Notched | 2.90 J/cm² | 13.8 ft-lb/in² | ISO 179 |
Menzolit Menzolit® BMC 0180 Unsaturated Polyester UP BMC 0180 is a general purpose BMC for electrical applications. Product according to type 803 DIN 16911. The glass content is on a level that combines good mould ability with good strength and stiffn.. |
|||
Charpy Impact, Notched | 2.90 J/cm² | 13.8 ft-lb/in² | ISO 179 |
Menzolit Menzolit® BMC 0200 Unsaturated Polyester UP BMC 0200 is a standard BMC for general purpose applications. The glass content is on a level that combines good mouldability with good strength and stiffness properties. Even without a specific fire.. |
|||
Charpy Impact, Notched | 2.90 J/cm² | 13.8 ft-lb/in² | ISO 179 |
Menzolit Menzolit® BMC 1650 Unsaturated Polyester UP BMC 1650 is a specially designed anti-microbial polyester moulding compound which incorporates a "germ killer" . It has been tested and found to be compliant for resistance to fungal defacement in .. |
|||
Charpy Impact, Notched | 2.90 J/cm² | 13.8 ft-lb/in² | ISO 179 |
Menzolit Menzolit® BMC 0190 Unsaturated Polyester UP BMC 0190 is a general purpose BMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The flammability me.. |
|||
Charpy Impact, Notched | 2.90 J/cm² | 13.8 ft-lb/in² | ISO 179 |
Menzolit Menzolit® BMC 0300 Unsaturated Polyester UP BMC 0300 is a low shrink standard material for general-purpose applications, which require a higher level on surface quality and better dimensional stability. The glass content is on a level that co.. |
|||
Charpy Impact, Notched | 2.90 J/cm² | 13.8 ft-lb/in² | ISO Data |
Styron Magnum™ 9555 ABS, High Impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact, Notched | 2.90 J/cm² @Temperature 23.0 °C |
13.8 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Noryl MX5569 PPE+PS PPE+PS blend. High Heat. Good balance of flow and impact. Offers good aging performance under heat. Typical applications include Automotive Interiors and Lighting.This data was supplied by SABIC-.. |
|||
Charpy Impact, Notched | 2.90 J/cm² | 13.8 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® FG50 NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 2.90 J/cm² | 13.8 ft-lb/in² | After conditioning at 23°C/50%RH; ISO 179/Af |
Arkema Group Orgalloy® LE 60 SF Polyamide Alloy Polyamide Alloy, Film and PackagingInformation provided by Arkema Group |
|||
Charpy Impact, Notched | 2.90 J/cm² | 13.8 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD4471 PC Lexan* HFD4471 is a 10% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4417 has enhanced mold release, impact ductili.. |
|||
Charpy Impact, Notched | 2.90 J/cm² | 13.8 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD4471 PC (Asia Pacific) Lexan* HFD4471 is a 10% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4417 has enhanced mold release, impact ductili.. |
|||
Charpy Impact, Notched | 2.90 J/cm² | 13.8 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD4471 PC (Europe-Africa-Middle East) Lexan* HFD4471 is a 10% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4417 has enhanced mold release, impact ductili.. |