Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 10.5 J/cm² | 50.0 ft-lb/in² | Partial Break; ISO 179/1eA |
Quadrant EPP Cesticolor™ HD 500 Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Charpy Impact, Notched | 10.5 J/cm² | 50.0 ft-lb/in² | Partial Break; ISO 179/1eA |
Quadrant EPP Cestidur™ Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Charpy Impact, Notched | 10.5 J/cm² | 50.0 ft-lb/in² | Partial Break; ISO 179/1eA |
Quadrant EPP Cestilene™ HD 500 Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Charpy Impact, Notched | 10.5 J/cm² | 50.0 ft-lb/in² | Partial Break; ISO 179-1/1eA |
Quadrant EPP PE 500 PE-HMW, virgin (ISO Data) This grade exhibits a good combination of stiffness, toughness, mechanical damping ability with wear- and abrasion resistance and can easily be welded. In less demanding applications with respect to.. |
|||
Charpy Impact, Notched | 10.5 J/cm² | 50.0 ft-lb/in² | Partial Break; ISO 179-1/1eA |
Quadrant EPP TIVAR® 1000 EC PE-UHMW + specific additives (ISO Data) TIVAR 1000 EC is a PE-UHMW grade containing specific additives rendering this material a lower surface resistivity than TIVAR 1000 antistatic, improving electrical conductivity and UV-resistance |
|||
Charpy Impact, Notched | 10.5 J/cm² | 50.0 ft-lb/in² | Partial Break; ISO 179-1/1eA |
Quadrant EPP TIVAR® Ceram P PE-UHMW + micro glass beads + other additives (ISO Data) TIVAR Ceram P is a wear improved PE-UHMW material with incorporated micro glass beads, specifically developed for use in the dewatering zone of paper machinery equipped with plastic wires and manufa.. |
|||
Charpy Impact, Notched | 10.5 J/cm² | 50.0 ft-lb/in² | Partial Break; ISO 179-1/1eA |
Quadrant EPP TIVAR® TECH PE-UHMW + MoS2 (ISO Data) This PE-UHMW grade with extremely high degree of polymerisation contains molybdenum disulphide, resulting in a material with improved wear resistance and sliding properties over TIVAR 1000. |
|||
Charpy Impact, Notched | 10.5 J/cm² | 50.0 ft-lb/in² | ISO 179 |
Manifattura Cattaneo PE HD Polyethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Charpy Impact, Notched | 10.5 J/cm² | 50.0 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST801AHS BK010 Nylon 66
(Unverified Data**) Super Toughened Heat Stabilized Polyamide 66 Zytel ST801AHS BK010 is a Super Tough high performance black polyamide 66 resin. It offers outstanding molding performance in injection molding applicati.. |
|||
Charpy Impact, Notched | 10.5 J/cm² @Temperature -30.0 °C |
50.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1eA |
Lanxess Durethan® BC 700 HTS 900116 Nylon 6/66
(discontinued **) PA 6/66 |