Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.70 J/cm² @Temperature 0.000 °C |
8.09 ft-lb/in² @Temperature 32.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY6414 PC (Asia Pacific) |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL A63 S15 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Geloy FXW751SK ASA+PC (Europe-Africa-Middle East) Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact ResinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® BPL1000 PC (Asia Pacific) Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® ML6430 PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Asia Pacifi.. |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO Data |
Americas Styrenics Styron® 482 High Impact Polystyrene
(discontinued **) STYRON® 482 high impact polystyrene resin is a high flow resin typically used in toys. When used unmodified for the manufacture of food contact articles STYRON 482 complies with the US Food, Drug a.. |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | |
Ineos ABS Lustran® QE 1455/L2, Injection Grade
(discontinued **) Injection molding grade, increased heat resistance, medium gloss, UV-stabilized grade.Applications: Automotive: body parts.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005.. |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | DIN 53453 |
IRPC Polimaxx Polene GA3245 High Density Polyethylene CHARACTERISTICS: HIGH TOUGHNESS, GOOD EXTRUDABILITY, EXCELLENT IMPACT STRENGTHAPPLICATIONS: BLOW FILM EXTRUSION FOR CARRIER BAGS, GROCERY BAGS, SHOPPING BAGS, INDUSTRIAL BAGS, LINER BAGS |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO 179/1eA |
Kuraray Genestarâ„¢ GX1500A-M41 Nylon, 50% Glass Filled 50% Glass reinforced injection grade. This grade was developed specifically for high mechanical properties for TD direction.Main Features:Low warpageHigh mechanical properties for TD directionExamp.. |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics LNP THERMOCOMP DX06313I PC (Asia Pacific) DX06313I is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility. |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO 179 |
Styrolution PS 495F HIPS Styrolution PS 495F is a high flow, high impact polystyrene with a good heat resistance and a high stiffness.High flow HIPSGood heat resistance with high stiffnessSuitable for gas-assisted injection.. |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO 179 |
Styrolution Terluran® HH-106 ABS Terluran HH-106 is an injection molding ABS grade with high resistance to heat deformation and impact.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL NH5120 PPE+PS Noryl* NH5120 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated V1 flame re.. |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO 179-1 |
Unitika E-RUNG60 PA66, 60% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 TLWCP Nylon 66, Flame Protection Grade V-2, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® XE 4107 nat PA612-GF40 Product description: Grilamid XE 4107 natural is a 40% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4107 are: low water absorptiong.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 30.0 °C |
8.09 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4128 black 9221 PA610 Product description: Grilamid XE 4128 black 9221 is a modified high viscosity Polyamide 610 for extrusion as well as injection molding. A characteristic of tubes made out of this material is the hig.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Delrin® 100STE NC010 Acetal (POM)
(Unverified Data**) Super Toughened High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100STE NC010 (formerly DE20590) is a high-viscosity super-toughened acetal homopolymer with very low VOC emissions. P.. |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 70G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Polyamide 66Zytel 70G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612
(Unverified Data**) 43% Glass Reinforced Polyamide 612Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 30.0 °C |
8.09 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® BGZ-30 PA6-GF30 Product description: Grilon BGZ-30 is a normal viscosity, heat stabilized and impact modified PA 6 injection molding type with 30% glass fibers. Grilon BGZ-30 has the following important properties:.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST801 BK010A Nylon 66
(Unverified Data**) Super Toughened Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | 1eA; ISO 179 |
Azoty Tarnow™ TARFLEN SG-2 PTFE Free-Flowing suspension powder for automated compression molding of complicated shapes and isostatic pressing.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | dry; ISO 179 1eA |
Azoty Tarnow™ Tarnamid® T-27 GF35 Polyamide 6 - Glass Fiber Reinforced 35% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO Data |
Styron Magnum™ 3490 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6
(Unverified Data**) 40% Glass Reinforced Toughened Polyamide 6 Zytel EFE7374 is a 40% fiber reinforced heat stabilized lubricated toughened polyamide 6 for injection molding. It has an improved impact resistance and ex.. |
|||
Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics GELOY FXW751SK ASA+PC Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact Resin |