Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.620 J/cm² | 2.95 ft-lb/in² | ISO 179/1eA |
Radici Radilon® SHS (dry) Nylon 6 General PurposeInformation provided by Radici group. |
|||
Charpy Impact, Notched | 0.620 J/cm² | 2.95 ft-lb/in² | EN ISO 179/1eA |
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced Main Charactistics: Stress resistant; High impact strength at 196 ° C Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInformation provided by Zedex |
|||
Charpy Impact, Notched | 0.620 J/cm² @Temperature -30.0 °C |
2.95 ft-lb/in² @Temperature -22.0 °F |
|
Eastman Eastar DN004 PCTG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Charpy Impact, Notched | 0.620 J/cm² | 2.95 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Crastin® CE15315 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin CE15315 NC010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0.. |
|||
Charpy Impact, Notched | 0.620 J/cm² @Temperature -30.0 °C |
2.95 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Crastin® CE15315 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin CE15315 NC010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0.. |
|||
Charpy Impact, Notched | 0.620 J/cm² | 2.95 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Rynite® FR515 BK507 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8m.. |
|||
Charpy Impact, Notched | 0.620 J/cm² @Temperature -30.0 °C |
2.95 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® PLS FR95G15DH2 BK269 Nylon 6 15% Glass Reinforced Flame Retardant Heat Stabilized Polyamide Zytel PLSFR95G15DH2 BK269 is 15% glass reinforced flame retardant black PA using SHIELD Technology only from DuPont exceptional resista.. |
|||
Charpy Impact, Notched | 0.620 J/cm² | 2.95 ft-lb/in² | ISO R179 |
Arkema Group ORGASOL® 1002 D Nat 1 Polyamide 6 Information provided by Arkema Group |
|||
Charpy Impact, Notched | 0.620 J/cm² | 2.95 ft-lb/in² | 1eA; ISO 179 |
Azoty Tarnow™ TARNOFORM 300 SI POM Tribological modified grade with silicon, for better sliding properties in plastic-plastic contact.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Charpy Impact, Notched | 0.620 J/cm² | 2.95 ft-lb/in² | ASTM D256 |
Plenco 7552 Phenolic, Nodular, Transfer Molded PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL re.. |
|||
Charpy Impact, Notched | 0.620 - 1.15 J/cm² | 2.95 - 5.47 ft-lb/in² | Average value: 0.919 J/cm² Grade Count:9 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |