Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.320 J/cm² | 1.52 ft-lb/in² | ISO 180 |
Nanocyl PLASTICYL™ PP2001 Polypropylene with 2 wt% Multi-Wall Carbon Nanotubes PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |
|||
Charpy Impact, Notched | 0.320 - 0.800 J/cm² | 1.52 - 3.81 ft-lb/in² | Average value: 0.607 J/cm² Grade Count:3 |
Overview of materials for PCT, 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr.. |
|||
Charpy Impact, Notched | 0.320 - 0.850 J/cm² | 1.52 - 4.05 ft-lb/in² | Average value: 0.475 J/cm² Grade Count:12 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Charpy Impact, Notched | 0.320 - 0.650 J/cm² @Temperature -30.0 - -30.0 °C |
1.52 - 3.09 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.443 J/cm² Grade Count:4 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Charpy Impact, Notched | 0.320 J/cm² @Temperature 23.0 °C |
1.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/1eA |
FKuR Kunststoff Terralene® WF 5525 Biobased Polyethylene With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol.. |
|||
Charpy Impact, Notched | 0.320 J/cm² | 1.52 ft-lb/in² | ISO 179/1eA |
Lucite International Diakon® ST25G6 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Charpy Impact, Notched | 0.320 J/cm² | 1.52 ft-lb/in² | ISO 179/1eA |
Lucite International Diakon® TD625 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Charpy Impact, Notched | 0.320 J/cm² | 1.52 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 50H1 PA66, DRY Description: Flame retardant polyamide 66, unreinforced, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This phospho.. |
|||
Charpy Impact, Notched | 0.320 J/cm² | 1.52 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® 2000 Polybutylene Terephthalate (PBT), High flow DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.320 J/cm² | 1.52 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® 2002 Polybutylene Terephthalate (PBT), Low friction, Low wear DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.320 J/cm² | 1.52 ft-lb/in² | ISO 179/1eA |
Polyplastics FR-PET® BLR6001MZ Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET) Information provided by PolyPlastics. |
|||
Charpy Impact, Notched | 0.320 J/cm² | 1.52 ft-lb/in² | EN ISO 179/1eA |
Wolf Kunststoff ZEDEX® ZX-100MT A1T Polymer Alloy, Mineral Reinforced Stiff; Hard; Very high strength; No fiber reinforcementApplications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automotive Technology, Machine ToolsInformation provided by Zed.. |
|||
Charpy Impact, Notched | 0.320 J/cm² @Temperature -20.0 °C |
1.52 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Xmod™ PC75 High Crystalline Polypropylene Copolymer Xmod PC75 is a HCPP intended for injection molding of automotive interior parts. Xmod PC75 is a very easy-flowing material combined with a good balance between impact strength and stiffness. The m.. |
|||
Charpy Impact, Notched | 0.320 J/cm² @Temperature 23.0 °C |
1.52 ft-lb/in² @Temperature 73.4 °F |
EN ISO 179 |
Ensinger TECASINT™ 2061 Polyimide, 15% Graphite, 10% PTFE Filled (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
Charpy Impact, Notched | 0.320 J/cm² | 1.52 ft-lb/in² | ISO 179 1eA |
Azoty Tarnow™ Tarnamid® T-27 GB30 Polyamide 6 - Glass Beads Reinforced 30% Glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Charpy Impact, Notched | 0.320 J/cm² | 1.52 ft-lb/in² | ASTM D256 |
Chang Chun Plastic Longlite PM T308J General Purpose Phenolic Molding Compound ASTM Grade per ASTM D700 is 3.Information provided by Dowell Trading Company Ltd. |
|||
Charpy Impact, Notched | 0.320 J/cm² | 1.52 ft-lb/in² | ASTM D256 |
Chang Chun Plastic Longlite PM T33J General Purpose Phenolic Molding Compound ASTM Grades per ASTM D700 are 2,3.Information provided by Dowell Trading Company Ltd. |
|||
Charpy Impact, Notched | 0.320 J/cm² | 1.52 ft-lb/in² | ASTM D256 |
Chang Chun Plastic Longlite PM T359J General Purpose Phenolic Molding Compound ASTM Grades per ASTM D700 are 3, 14.Information provided by Dowell Trading Company Ltd. |
|||
Charpy Impact, Notched | 0.320 J/cm² | 1.52 ft-lb/in² | ASTM D256 |
Chang Chun Plastic Longlite PM T376J Heat Resistant Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Charpy Impact, Notched | 0.320 J/cm² | 1.52 ft-lb/in² | 1eA; ISO 179 |
Azoty Tarnow™ TARNOFORM 300 DW POM Tribological modified grade with combination of damping and wear reducing additives. Finished parts have low coefficient of friction and wear with reduction of acoustic emission during sliding.Infor.. |
|||
Charpy Impact, Notched | 0.320 J/cm² | 1.52 ft-lb/in² | ASTM D256 |
Chang Chun Plastic Longlite PM T385J General Purpose Phenolic Molding Compound ASTM Grades per ASTM D700 are 2, 3.Information provided by Dowell Trading Company Ltd. |
|||
Charpy Impact, Notched | 0.320 - 0.860 J/cm² | 1.52 - 4.09 ft-lb/in² | Average value: 0.674 J/cm² Grade Count:19 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |