Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.270 J/cm² @Temperature 23.0 °C |
1.28 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
Hexion Bakelite™ PF 51 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Contact support power switch, switch.. |
|||
Charpy Impact, Notched | 0.270 - 1.00 J/cm² @Temperature -40.0 - -20.0 °C |
1.28 - 4.76 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 0.734 J/cm² Grade Count:10 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Charpy Impact, Notched | 0.270 J/cm² @Temperature -23.0 °C |
1.28 ft-lb/in² @Temperature -9.40 °F |
DIN 53453 |
Global PP-1100-NK Polypropylene Homopolymer Description-transparency, high stiffness, high heat resistantApplications-general purpose, household goods, closures, food applicationsInformation provided by Global Polymers Corporation. |
|||
Charpy Impact, Notched | 0.270 J/cm² @Temperature -20.0 °C |
1.28 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
Global PP-2340-S Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-electrical appliances, bases, panels, auto parts, cupsInformation provided by Global Polymers Corpo.. |
|||
Charpy Impact, Notched | 0.270 J/cm² | 1.28 ft-lb/in² | ISO 179/1eA |
Lucite International Diakon® CRG800 Acrylic Polymer, Toughened Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Charpy Impact, Notched | 0.270 J/cm² | 1.28 ft-lb/in² | ISO 179 |
Sumitomo Bakelite North America RX® 660 Fiberglass Reinforced Phenolic Novolac RX 660 is a fiberglass reinforced phenolic molding compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type MFH.Information supplied by Sumitom.. |
|||
Charpy Impact, Notched | 0.270 J/cm² | 1.28 ft-lb/in² | ASTM D256 |
Plenco 6553 Phenolic, Granular, Compression Molded Two-Stage Phenolic. PLENCO 06553 is a phenolic molding compound, formulated specifically for automotive brake pistons. 06553 exhibits excellent dimensional stability, and resistance to brake fluids.. |
|||
Charpy Impact, Notched | 0.270 J/cm² | 1.28 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® 500FP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.270 J/cm² | 1.28 ft-lb/in² | ISO 179-1 |
Vyncolit X655/1 Glass Fiber and Mineral Filled Novolac Phenolic Novolac resin based, glass fiber and mineral filled. High dimensional stability and excellent chemical resistance at high temperatures in hydraulic brake fluids. Used in particular in the ABS system.. |
|||
Charpy Impact, Notched | 0.270 J/cm² | 1.28 ft-lb/in² | ISO 179-1 |
Vyncolit X655RB Glass Fiber and Mineral Filled Novolac Phenolic Novolac resin based, glass fiber and mineral reinforced. Grade with superior stiffness, high dimensional stability and high wear resistance. Good chemical resistance against several fuels at elevate.. |
|||
Charpy Impact, Notched | 0.270 J/cm² @Temperature -30.0 °C |
1.28 ft-lb/in² @Temperature -22.0 °F |
|
Eastman Eastapak 9921 PET ISO data as provided by the manufacturer, Eastman Chemical |
|||
Charpy Impact, Notched | 0.270 J/cm² | 1.28 ft-lb/in² | |
Eastman Eastar EN058 PET Copolymer ISO data as provided by the manufacturer, Eastman Chemical |
|||
Charpy Impact, Notched | 0.270 J/cm² | 1.28 ft-lb/in² | ISO 179 |
Chi Mei Kibiton® PB-5910 SBC High transparency, medium stiffness, toughness |
|||
Charpy Impact, Notched | 0.270 J/cm² | 1.28 ft-lb/in² | |
Biomer P226 PHB Biodegradable Polymer PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula of the subunit is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. P.. |
|||
Charpy Impact, Notched | 0.270 J/cm² @Temperature -30.0 °C |
1.28 ft-lb/in² @Temperature -22.0 °F |
ISO data |
BASF Capron® 8260 40% Mineral-Filled Nylon 6 (Dry)
(discontinued **) Capron 8260 is a 40% mineral reinforced polyamide 6 injection molding compound. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability includi.. |
|||
Charpy Impact, Notched | 0.270 - 0.500 J/cm² @Temperature -30.0 - -30.0 °C |
1.28 - 2.38 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.345 J/cm² Grade Count:4 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |
|||
Charpy Impact, Notched | 0.270 J/cm² @Temperature 23.0 °C |
1.28 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Conditioned) Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.Information provided by BASF |