Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.170 - 2.00 J/cm²
0.809 - 9.52 ft-lb/in²
Average value: 0.756 J/cm² Grade Count:123
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15..
Charpy Impact, Notched 0.170 J/cm²

@Temperature -30.0 °C
0.809 ft-lb/in²

@Temperature -22.0 °F
Ineos ABS Centrex® 815 ASA Blend  (discontinued **)
Key Features:UnfilledLight stabilized or stable to lightU.V. stabilized or stable to weatherHeat stabilized or stable to heatSuitable processing methods:Injection moldingInformation provided by Baye..
Charpy Impact, Notched 0.170 - 0.210 J/cm²
0.809 - 0.999 ft-lb/in²
Average value: 0.188 J/cm² Grade Count:4
Overview of materials for Phenolic, Novolac, Heat Resistant Grade, Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Heat Resistant Grade, Filled". Each property range of values reported is minimum and ..
Charpy Impact, Notched 0.170 J/cm²
0.809 ft-lb/in²
ASTM D256
Plenco 4100 Phenolic, Granular, Injection Molded  (discontinued **)
Two-stage Phenolic. PLENCO 04100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability characteristics and molded finish. It is used in appliance and ..
Charpy Impact, Notched 0.170 J/cm²
0.809 ft-lb/in²
ASTM D256
Plenco 4246 Phenolic, Granular, Injection Molded  (discontinued **)
Two-stage Phenolic. PLENCO 04246 flow 18 is a black two-stage, medium heat resistant phenolic molding compound. It has excellent electrical, moldability and molded finish characteristics. It is use..
Charpy Impact, Notched 0.170 J/cm²
0.809 ft-lb/in²
J/cm; ASTM D256
Plenco Valite 1246-18X Novolac Phenolic, Granular, Injection Molded  (discontinued **)
This Valite product has been replaced by Plenco 4246. Data provided by Plenco.VALITE 1246-18X is a black two-stage, medium heat resistant phenolic molding compound. It has excellent electrical, mol..
Charpy Impact, Notched 0.170 J/cm²
0.809 ft-lb/in²
J/cm; ASTM D256
Plenco Valite 4100 Novolac Phenolic, Granular, Injection Molded  (discontinued **)
This Valite product has been replaced by Plenco 4100. Data provided by Plenco.VALITE 4100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability charac..
Charpy Impact, Notched 0.170 J/cm²
0.809 ft-lb/in²
ISO 179/1eA
Lucite International Diakon® Frost 902 51 Acrylic Polymer
Information provided by Lucite International
Charpy Impact, Notched 0.170 J/cm²

@Temperature 23.0 °C
0.809 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Topas Advanced Polymers TOPAS® 6013M-07 Cyclic Olefin Copolymer (COC)
TOPAS® 6013M-07 is an injection molding grade with a wide processing window, especially suited for blow molding processes including IBM and ISBM. It is a glass-clear amorphous polymer with outstand..
Charpy Impact, Notched 0.170 J/cm²

@Temperature -30.0 °C
0.809 ft-lb/in²

@Temperature -22.0 °F
BASF Novolen® 1184 L Polypropylene
Nucleated grade with high processing stability containing antistatic for thermoformed parts.Data was collected by ISO methods and provided by BASF.
Charpy Impact, Notched 0.170 J/cm²

@Temperature -30.0 °C
0.809 ft-lb/in²

@Temperature -22.0 °F
BASF Novolen® 1102 K Polypropylene
Grade with high processing stability for film tape (low water carryover), fibrillated film, monofilaments, OPP film (special formulations) and thermoformed parts.Data was collected by ISO methods an..
Charpy Impact, Notched 0.170 J/cm²

@Temperature -30.0 °C
0.809 ft-lb/in²

@Temperature -22.0 °F
BASF Novolen® 1104 K Polypropylene
Data was collected by ISO methods and provided by BASF.
Charpy Impact, Notched 0.170 - 1.00 J/cm²
0.809 - 4.76 ft-lb/in²
Average value: 0.442 J/cm² Grade Count:17
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..