Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 65.0 MPa | 9430 psi | ISO 2039-1 |
Quadrant EPP Symalit® 1000 ECTFE, unfilled, lining industries (ISO Data) Symalit 1000 ECTFE is made from a fluoropolymer resin that is a copolymer of ethylene and chlorotrifluoroethylene. It exhibits good mechanical properties combined with an excellent chemical resistan.. |
|||
Ball Indentation Hardness | 65.0 - 105 MPa | 9430 - 15200 psi | Average value: 90.0 MPa Grade Count:7 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Ball Indentation Hardness | 65.0 MPa | 9430 psi | ISO 2039-1 |
Ineos ABS Lustran® ABS E112LG Pellets Lustran® ABS E112LG is extrusion grade for low gloss surfaces. It is used for the production of molded plastic articles. |
|||
Ball Indentation Hardness | 65.0 MPa @Load 36.5 kg, Time 30.0 sec |
9430 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Styrolution Luran® S 796 M Colored ASA Description: High-impact injection molding gr4ade with good flowability.Applications: Trim panels for goods vehicles.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Ball Indentation Hardness | 65.0 MPa @Load 36.5 kg, Time 30.0 sec |
9430 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Styrolution Luran® S 797 S UV White 33999 Q455 ASA Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Ball Indentation Hardness | 65.0 MPa @Load 36.5 kg, Time 30.0 sec |
9430 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Styrolution Luran® S 797 S White 35962 ASA Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Ball Indentation Hardness | 65.0 MPa | 9430 psi | ISO 2039-1 |
Styrolution PS 2710 HIPS Styrolution PS 2710 is a high impact grade of polystyrene with improved stress crack resistance, developed for extrusion and thermoforming applications, especially for the refrigerator industry.Impr.. |
|||
Ball Indentation Hardness | 65.0 MPa | 9430 psi | 358 N/30s; ISO 2039 |
Borealis HB601WG Polypropylene Homopolymer HB601WG is a polypropylene homopolymer intended for injection molding and blow molding. The product is available in natural but other colors can be provided on request. This material has excellent .. |
|||
Ball Indentation Hardness | 65.0 MPa | 9430 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSS/4 LF 1 PA666 Product description: Grilon TSS/4 LF 1 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 1% lubricant (molybdenum disulphide). Grilon TSS/4 LF 1 has the following import.. |
|||
Ball Indentation Hardness | 65.0 MPa | 9430 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSS/4 LF 2 PA666 Product description: Grilon TSS/4 LF 2 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 2% lubricant (molybdenum disulphide). Grilon TSS/4 LF 2 has the following import.. |
|||
Ball Indentation Hardness | 65.0 MPa | 9430 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSS/4 PA666 Product description: Grilon TSS/4 is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS/4 has the following important properties: Good flow behaviorEas.. |
|||
Ball Indentation Hardness | 65.0 MPa @Load 36.5 kg, Time 30.0 sec |
9430 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultraform® N2650 Z6 (LEV) POM Description: Is a POM + PUR, elastomer-modified injection-molding grade for applications requiring the highest impact strength together with low stiffness.Information provided by BASF |
|||
Ball Indentation Hardness | 65.0 - 70.0 MPa | 9430 - 10200 psi | DIN 53 456 |
Isoflon PCTFE Polychlorotrifluoroethylene Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Ball Indentation Hardness | 65.0 MPa | 9430 psi | Fm=358N; Ø 50x4mm; ISO 2039-1 |
SYNTHOS Krasten® 562E High Impact Polystyrene High impact grade with properties suitable for thermoforming. Processed mainly by extrusion and thermoforming. Production of plates, sheets, technical parts and molded packaging (used in e.g. the fo.. |