Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 40.0 MPa | 5800 psi | |
Murtfeldt Original Material ”S”® plus + FP Polyethylene Original Material ”S”® plus+ FP [FS] is a technical plastic that completely meets the requirements of the food sector for the detectability of plastic foreign bodies in foods. “FP” stands for “.. |
|||
Ball Indentation Hardness | 40.0 MPa | 5800 psi | ISO2039.1 DIN.53456 |
Omnia Plastica PE 1000 - Polyethylene 1000 Polyethylene with a molecular weight of ± 1000,000 with excellent impact strength. PE 1000 is less rigid and has a higher shock resistance than the low molecular weight polyethylene and it is there.. |
|||
Ball Indentation Hardness | 40.0 MPa | 5800 psi | ISO 2039-1 |
Quadrant EPP Cestilene™ HD 1000 R Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Ball Indentation Hardness | 40.0 MPa | 5800 psi | ISO 2039-1 |
Quadrant EPP Fluorosint® 207 PTFE + mica, compression moulded (ISO Data) This material has a food contact compliant composition which, in combination with the good mechanical performance, dimensional stability, sliding and wear properties and inherent outstanding chemica.. |
|||
Ball Indentation Hardness | 40.0 MPa | 5800 psi | ISO 2039-1 |
Quadrant EPP Semitron® ESd 500HR PTFE, static dissipative, extruded (ISO Data) Reinforced with a proprietary synthetic mica, Semitron ESd 500HR offers an excellent combination of low frictional properties, good dimensional stability and electrostatic dissipation. Whenever virg.. |
|||
Ball Indentation Hardness | 40.0 - 135 MPa | 5800 - 19600 psi | Average value: 75.0 MPa Grade Count:5 |
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Mica Filled". Each property range of values reported is minimum and maxi.. |
|||
Ball Indentation Hardness | 40.0 MPa | 5800 psi | ASTM 1457-62 T |
Fluorseals PTFE 60% bronze filled Improved compressive strength and thermal conductivity.Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials. |
|||
Ball Indentation Hardness | 40.0 MPa | 5800 psi | H385/30; ISO 2039 |
Borealis Daplen™ EG102AI Polypropylene Compound 15% Mineral Filled Daplen EF102AI is a 15% mineral filled polypropylene compound intended injection molding. EG102AI is an easy flow grade, specially developed for the car industry. Daplen EF102AI has been developed.. |
|||
Ball Indentation Hardness | 40.0 MPa | 5800 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BFZ 3 PA6 Product description: Grilon BFZ 3 is an unreinforced, high impact resistant PA6 extrusion grade. Grilon BFZ 3 has the following important properties: Extreme toughnessEasy processingLow density Gril.. |
|||
Ball Indentation Hardness | 40.0 MPa | 5800 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BZ 3 PA6 Information provided by EMS Grivory |
|||
Ball Indentation Hardness | 40.0 MPa | 5800 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® EB 50 H DZ PA6 Product description: Grilon EB 50 H DZ is a high viscosity, unreinforced, heat stabilized, impact modified PA6 extrusion blow molding grade. Grilon EB 50 H DZ has the following important properties:.. |
|||
Ball Indentation Hardness | 40.0 MPa | 5800 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® L 25 W 20 PA12 Product Description: Grilamid L 25 W 20 is a semi-flexible plasticized high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 20 is UV and heat stabilized. The main features of Grila.. |
|||
Ball Indentation Hardness | 40.0 MPa | 5800 psi | ISO 2039-1 |
Azoty Tarnow™ TARFLEN SM-B40 PTFE Reinforced with 40% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Ball Indentation Hardness | 40.0 - 44.0 MPa | 5800 - 6380 psi | ISO 2032 |
Adamas Adalon® 826 PTFE, 50% Stainless steel Information provided by Adamas, HPM |
|||
Ball Indentation Hardness | 40.0 - 46.0 MPa | 5800 - 6670 psi | ISO 2032-N132 |
Adamas Adalon® 503 PTFE, 0.1% MoS2 Information provided by Adamas, HPM |
|||
Ball Indentation Hardness | 40.0 MPa | 5800 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® XE 4208 black 9992 PA612-I Product description: Grilamid XE 4208 black 9992 is a semiflexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) extrusion grade. Unique properties of Gril.. |
|||
Ball Indentation Hardness | 40.0 MPa | 5800 psi | value at 30 sec.; ISO 2039-1 |
CENTROPLAST CENTROLEN PE-UHMW Ultra-high molecular weight polyethylene This plastic is a low density, easily machined material that can be welded and has a low sliding friction with high impact resistance. Applications include glide strips, pump components, and wearin.. |