Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 360 MPa | 52200 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® GVX-7 H black 9915 PA*-GF70 Product description: Grivory GVX-7H black 9915 is a 70% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Ball Indentation Hardness | 360 MPa | 52200 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® GVX-7 H nat PA*-GF70 Product description: Grivory GVX-7H natural is a 70% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamid.. |
|||
Ball Indentation Hardness | 360 MPa | 52200 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® HTV-6H1 black 9205 PA6T/6I-GF60 Product description: Grivory HTV-6H1 black 9205 is a 60% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
Ball Indentation Hardness | 360 MPa | 52200 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® HTV-6H1 black 9205 PA6T/6I-GF60 Product description: Grivory HTV-6H1 black 9205 is a 60% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
Ball Indentation Hardness | 360 MPa | 52200 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® HTV-6H1 nat PA6T/6I-GF60 Product description: Grivory HTV-6H1 natural is a 60% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac.. |
|||
Ball Indentation Hardness | 360 MPa | 52200 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® HTV-6H1 nat PA6T/6I-GF60 Product description: Grivory HTV-6H1 natural is a 60% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac.. |
|||
Ball Indentation Hardness | 360 MPa | 52200 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GV XE 16102 (GVL-6H HP) PA*-GF60 Product description: Grivory XE 16102 natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long special glass fibers. Grivory.. |
|||
Ball Indentation Hardness | 360 MPa | 52200 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® HT1V-6 FWA black 9225 PA6T/6I-GF60 Product description: Grivory HT1V-6 FWA black 9225 is a 60 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |
|||
Ball Indentation Hardness | 360 MPa | 52200 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® HT1V-6 FWA black 9225 PA6T/6I-GF60 Product description: Grivory HT1V-6 FWA black 9225 is a 60 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |
|||
Ball Indentation Hardness | 360 MPa | 52200 psi | H 961/30; ISO 2039-1 |
Akro-Plastic Akromid® T1 GF 50 (3101) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |