Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 280 MPa | 40600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BGZ-50/2 PA6-I-GF50 Information provided by EMS Grivory |
|||
Ball Indentation Hardness | 280 MPa | 40600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GC-4H PA*-CF40 Product description: Grivory GC-4H is a 40% carbon-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamide. Grivo.. |
|||
Ball Indentation Hardness | 280 MPa | 40600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GV-5 FWA black 9225 PA*-GF50 Product description: Grivory GV-5 FWA black 9225 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copoly.. |
|||
Ball Indentation Hardness | 280 MPa | 40600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GV-5H black PA*-GF50 Product description: Grivory GV-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Ball Indentation Hardness | 280 MPa | 40600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GV-5H EF black 9915 PA*-GF50 Product description: Grivory GV-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Ball Indentation Hardness | 280 MPa | 40600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GV-5H EF nat PA*-GF50 Product description: Grivory GV-5H EF natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyam.. |
|||
Ball Indentation Hardness | 280 MPa | 40600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GV-5H PA*-GF50 Product description: Grivory GV-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide.. |
|||
Ball Indentation Hardness | 280 MPa | 40600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GVS-5H nat PA*-GF50 Product description: Grivory GVS-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide.. |
|||
Ball Indentation Hardness | 280 MPa | 40600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® HTV-3H1 black 9205 PA6T/6I-GF30 Product description: Grivory HTV-3H1 black 9205 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
Ball Indentation Hardness | 280 MPa | 40600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® HTV-3H1 nat PA6T/6I-GF30 Product description: Grivory HTV-3H1 natural is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac.. |
|||
Ball Indentation Hardness | 280 MPa | 40600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSG-50/4 FA PA666-GF50 Information provided by EMS Grivory |
|||
Ball Indentation Hardness | 280 MPa | 40600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSG-50/4 PA666-GF50 Product description: Grilon TSG-50/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers. Grilon TSG-50/4 has the following important properties: High sti.. |
|||
Ball Indentation Hardness | 280 MPa | 40600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSGL-40/4 black 9833 PA666-GF40 Product description: Grilon TSGL-40/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 black is characterized by the following key-p.. |
|||
Ball Indentation Hardness | 280 MPa | 40600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSGL-40/4 FA black 9840 PA666-GF40 Product description: Grilon TSGL-40/4 FA black 9840 is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 FA black 9840 is characterized by th.. |
|||
Ball Indentation Hardness | 280 MPa | 40600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® XE 4095 black 9225 PA*-GF50 Product description: Grivory XE 4095 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Ball Indentation Hardness | 280 MPa | 40600 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® XE 4095 black 9225 PA*-GF50 Product description: Grivory XE 4095 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Ball Indentation Hardness | 280 MPa | 40600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GVS-5H black 9915 PA*-GF50 Product description: Grivory GVS-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Ball Indentation Hardness | 280 MPa | 40600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® HT1V-3 FWA black 9225 PA6T/6I-GF30 Product description: Grivory HT1V-3 FWA black 9225 is a 30 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |
|||
Ball Indentation Hardness | 280 MPa | 40600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® HT1V-3 FWA nat PA6T/6I-GF30 Product description: Grivory HT1V-3 FWA natural is a 30 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6.. |
|||
Ball Indentation Hardness | 280 MPa | 40600 psi | H 961/30; ISO 2039-1 |
Akro-Plastic Akromid® B3 GF 50 RM-M (3146) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Ball Indentation Hardness | 280 MPa | 40600 psi | H 961/30; ISO 2039-1 |
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Ball Indentation Hardness | 280 MPa | 40600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GV-5 FWA nat PA*-GF50 Product description: Grivory GV-5 FWA natural is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Ball Indentation Hardness | 280 MPa | 40600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® HT1V-3 HY black 9205 PA6T/6I-GF30 Product description: Grivory HT1V-3 HY black 9205 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-3 HY bl.. |