Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 62.0 MPa | 8990 psi | DIN 53456 |
Ineos Nova S-4600 High Impact Compact Polystyrene
(discontinued **) High impact polystyrene with excellent flow characteristics, a very high toughness and a high elongation. Main application are injection molding of technical parts and housings. For injection mold.. |
|||
Ball Indentation Hardness | 62.0 - 106 MPa | 8990 - 15400 psi | Average value: 85.5 MPa Grade Count:15 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Ball Indentation Hardness | 62.0 - 105 MPa | 8990 - 15200 psi | Average value: 92.5 MPa Grade Count:4 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Ball Indentation Hardness | 62.0 - 68.0 MPa | 8990 - 9860 psi | DIN 53 456 |
Isoflon PVDF Polyvinyl Dichloride Fluoropolymer Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Ball Indentation Hardness | 62.0 MPa @Load 36.5 kg, Time 30.0 sec |
8990 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Styrolution Terblend® N NG-02 EF 8% Glass Filled ABS+PA (Conditioned) Description: Terblend® N NG-02 EF is a glass fiber reinforced UV stabilized ABS/PA blend with excellent dimensional stability and high impact strength. The enhanced flowability enables excellent .. |
|||
Ball Indentation Hardness | 62.0 MPa | 8990 psi | 358 N/30s; ISO 2039 |
Borealis ME266U Polypropylene Compound, Mineral Filled ME266U is a 20% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and gives a good surface quality. .. |
|||
Ball Indentation Hardness | 62.0 MPa | 8990 psi | H 385/30; ISO 2039 |
Borealis Xmod™ BE677AI High Crystalline Polypropylene Copolymer Xmod BE677AI is a UV-stabilized HCPP intended for injection molding of automotive interior and appliance parts. Xmod BE677AI has an excellent balance between impact strength and stiffness as well .. |
|||
Ball Indentation Hardness | 62.0 MPa | 8990 psi | H 385/30; ISO 2039 |
Borealis Xmod™ MC55 High Crystalline Polypropylene Copolymer Xmod MC55 is a HCPP intended for injection molding of automotive interior parts. Xmod MC55 has an excellent balance between impact strength and stiffness as well as good surface quality.Xmod MC55 h.. |
|||
Ball Indentation Hardness | 62.0 MPa | 8990 psi | value at 30 sec.; ISO 2039-1 |
CENTROPLAST CENTROLEN PPS Polypropylene flame resistant This material is a low density, easily machined plastic that can be welded and is flame resistant. Applications include exhaust systems for heating systems, and apparatus engineering.Information pr.. |
|||
Ball Indentation Hardness | 62.0 - 99.0 MPa | 8990 - 14400 psi | Average value: 85.3 MPa Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |