Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 120 MPa | 17400 psi | ISO 2039-1 |
Nilit FRIANYL A63 E Raw extruded nylon 6.6 for injection molding Raw extruded nylon 6.6 for injection molding (available only in nature).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 120 MPa | 17400 psi | ISO 2039-1 |
Nilit FRIANYL A63 RV0 9005 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, flame retardant, halogen and phosphorus free.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 120 MPa | 17400 psi | ISO 2039-1 |
Nilit FRIANYL A63 RV0 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, flame retardant, halogen and phosphorus free.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 120 MPa | 17400 psi | ISO 2039-1 |
Quadrant EPP Nylatron® 703XL PA 6 + internal lubricant, cast (ISO Data) This high performance cast nylon 6 bearing grade provides an even better wear resistance than Nylatron NSM, combined with good pressure-velocity capabilities and a near zero level of “stick-slip”... |
|||
Ball Indentation Hardness | 120 MPa | 17400 psi | ISO 2039-1 |
Quadrant EPP Quadrant PC 1000 extruded (ISO Data) Quadrant Engineering Plastic Products is marketing non-UV-stabilized polycarbonate stock shapes under the trade name Quadrant PC 1000. It is a natural, “non-optical” industrial quality (clear, tra.. |
|||
Ball Indentation Hardness | 120 MPa | 17400 psi | DIN 53456 |
Ineos Nova S-2200 Medium Impact Compact Polystyrene
(discontinued **) Medium impact easy flowing polystyrene, designed for injection molding applications with short cycle times and for complicated technical parts. The product has a high stiffness and an excellent the.. |
|||
Ball Indentation Hardness | 120 MPa | 17400 psi | DIN 53456 |
Ineos Nova S-4200 Medium Impact Compact Polystyrene
(discontinued **) Medium impact polystyrene which combines excellent flow characteristics with a good dimensional stability under heat and a high stiffness. This grade is designed for injection molding of technical.. |
|||
Ball Indentation Hardness | 120 - 370 MPa | 17400 - 53700 psi | Average value: 203 MPa Grade Count:9 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Ball Indentation Hardness | 120 MPa | 17400 psi | ISO 2039 |
GEHR Plastics PC Polycarbonate Polycarbonate shows a high rigidity and an extreme impact strength. Also it has a high glass transition temperature and temperature resistance. The operating temperature ranges from -60°C to appr.. |
|||
Ball Indentation Hardness | 120 MPa | 17400 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics LAMIGAMID® 510 Polyethylene Terephthalate Application: friction bearings, wear linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 120 MPa | 17400 psi | ISO 2039-1 |
Styrolution Novodur® M205FC ABS Novodur HD M205FC is an injection molding grade especially suitable for medical applications providing enhanced stiffness.Information provided by Styrolution |
|||
Ball Indentation Hardness | 120 MPa | 17400 psi | ISO 2039-1 |
Styrolution PS 542N HIPS Styrolution PS 542N is an impact polystyrene with high heat resistance.Information provided by Styrolution |
|||
Ball Indentation Hardness | 120 MPa | 17400 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® 2SV-30H black 9992 PA610-GF30 Product Description: GRILAMID XE 3976 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mate.. |
|||
Ball Indentation Hardness | 120 MPa | 17400 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BG-40 FC PA6-GF40 Product description: Grilon BG-40 FC is a heat stabilized PA6 injection molding grade with 40% glass fibers. Grilon BG-40 FC has the following important properties: High stiffnessExcellent surface f.. |
|||
Ball Indentation Hardness | 120 MPa | 17400 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BT 40 Z PA6 Product description: Grilon BT 40 Z is an unreinforced, normal viscosity, impact modified polyamide blend with amorphous and semi-crystalline components. Grilon BT 40 Z has the following important p.. |
|||
Ball Indentation Hardness | 120 MPa | 17400 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® LV-30H FWA black 9225 PA12-GF30 Product description: Grilamid LV-30H FWA black 9225 is a 30 % glass fiber reinforced, heat stabilized polyamide12 injection molding grade with the following special features: Stiffness combined with.. |
|||
Ball Indentation Hardness | 120 MPa | 17400 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® LV-30H FWA nat PA12-GF30 Product description: Grilamid LV-30H FWA natural is a 30 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined with h.. |
|||
Ball Indentation Hardness | 120 MPa | 17400 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® LV-3A H PA12-GF30 Grilamid LV-3A H is a 30 % glass fibre reinforced PA12 for injection moulding. Grilamid LV-3A H is very stiff and tough and offers an improved hydrolysis resistance compared to standard PA12 GF 30.I.. |
|||
Ball Indentation Hardness | 120 MPa | 17400 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSC-30/4 LF 15 black 9832 PA666-(CF+Z)45 Product description: Grilon TSC-30/4 LF 15 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% carbon fibers and 15% of a combination of PTFE and silicone oil. Grilon .. |
|||
Ball Indentation Hardness | 120 MPa | 17400 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TR 55 PA12/MACMI Product description: Grilamid TR 55 natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 55 natural offers outstanding properties.. |
|||
Ball Indentation Hardness | 120 MPa | 17400 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TR 90 TL PAMACM12 Product description: Grilamid TR 90 TL is a transparent thermoplastic polyamide based on aliphatic, cycloaliphatic and aromatic blocks. The special characteristic of Grilamid TR 90 TL is the high st.. |
|||
Ball Indentation Hardness | 120 MPa | 17400 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® XE 5004 (BM-30/2 UV) PA666-MD30 Product description: Grilon XE 5004 is a normal viscosity PA6 injection molding grade with 30% mineral reinforcement, which is additionally UV stabilized. Grilon XE 5004 has the following important .. |
|||
Ball Indentation Hardness | 120 - 135 MPa | 17400 - 19600 psi | ISO 2032 |
Adamas Adalon® 452 PTFE, Mica filler Information provided by Adamas, HPM |
|||
Ball Indentation Hardness | 120 MPa @Load 36.5 kg, Time 30.0 sec |
17400 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultraform® N2520 L POM Description: Is a POM, product having reduced electric surface resistance.Information provided by BASF |
|||
Ball Indentation Hardness | 120 MPa | 17400 psi | value at 30 sec.; ISO 2039-1 |
CENTROPLAST CENTROMID 12 GF 30 Polyamide 12 30% glass fiber CENTROMID 12 GF 30 is a dimensionally stable and high strength material with good electrical insulating properties. Its applications include levers and valve parts.Information provided by CENTROPLA.. |
|||
Ball Indentation Hardness | 120 MPa | 17400 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® XE 4192 black 9992 PA610-GF30 Information provided by EMS Grivory |
|||
Ball Indentation Hardness | 120 MPa | 17400 psi | ISO 2039 |
GEHR Plastics PVC-U Polyvinylchloride Polyvinyl chloride is a flame retardant material with an exceptional chemical resistance and also with lower stress cracking. PVC-U shows high mechanical strength, tensile strength and the continuou.. |
|||
Ball Indentation Hardness | 120 MPa | 17400 psi | value at 30 sec.; ISO 2039-1 |
CENTROPLAST CENTRODAL TF Polyoxymethylene + PTFE This material is high strength and high heat strength dimensional stability. Applications include racks and annular gears, dimensionally accurate structural components for pumps, and housings and t.. |
|||
Ball Indentation Hardness | 120 MPa @Load 36.5 kg, Time 30.0 sec |
17400 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Styrolution Luran® S KR 2867 C WU Colored ASA+PC Description: Easy flowing injection molding grade containing bromine-, chlorine- and antimony-free flame retardant.Information provided by STYROLUTION, which is a joint venture between BASF and INEO.. |