Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 115 MPa | 16700 psi | ISO 2039-1 |
Nilit FRIANYL B63 H-TF20 Nylon 6 for injection molding, 20% PTFE lubricated Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | ISO 2039-1 |
Nilit FRIANYL B63 TF20 Nylon 6 for injection molding, 20% PTFE lubricated Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | ISO 2039-1 |
Nilit FRIANYL B63 HS-KV30 Nylon 6 for injection molding, 30% glass ball reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 115 - 116 MPa | 16700 - 16800 psi | Average value: 115 MPa Grade Count:4 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Ball Indentation Hardness | 115 - 227 MPa | 16700 - 32900 psi | Average value: 153 MPa Grade Count:11 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics LAMIGAMID® 307 Cast Polyamide 6, Heat Stabilized, Conditioned Application: slippers, inserts for coupling boxesInformation provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | ISO 2039-1 |
Styrolution Novodur® H802 ABS Novodur H802 is a high heat injection molding grade with high stiffness, especially suitable for being painted.Information provided by Styrolution |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | H 358/30; ISO 2039; DIN 53456 |
Zell-Metall Engineering Plastics Zellamid 900 (POM-C) Zellamid® 900 is the registered trademark of Zell-Metalls high molecular weight Acetal resin.Acetal (POM) is noted for its high mechanical strength, heat resistance and good antifriction .. |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | ISO 2039-1 |
Covestro Apec® 1603 High-Heat Polycarbonate This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along.. |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | ISO 2039-1 |
Covestro Makrolon® 1952 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Me.. |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | ISO 2039-1 |
Covestro Makrolon® 2256 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | ISO 2039-1 |
Covestro Makrolon® 2258 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | ISO 2039-1 |
Covestro Makrolon® 2405 MAS048 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | ISO 2039-1 |
Covestro Makrolon® 2652 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | ISO 2039-1 |
Covestro Makrolon® 2665 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medium viscosity, easy.. |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | ISO 2039-1 |
Covestro Makrolon® 2805 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | ISO 2039-1 |
Covestro Makrolon® 2805 MAS152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | ISO 2039-1 |
Covestro Makrolon® 6255 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Lo.. |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | ISO 2039-1 |
Covestro Makrolon® FS 2000 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Low viscosityAs of 1 S.. |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BG-35 S PA6-GF35 Information provided by EMS Grivory |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BKZ-30 PA6-GB30 Information provided by EMS Grivory |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® LV-23 X ESD PA12-GF23 Product description: Grilamid LV-23 X ESD black is an antistatic Polyamide 12 injection moulding grade with 23 % glass fibre reinforcement. Main attributes are: antistatic with reisitivity < 10^6 O.. |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSG-35/4 PA666-GF35 Product description: Grilon TSG-35/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers. Grilon TSG-35/4 has the following important properties: Good flo.. |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSG-35/4 W black 9832 PA666-GF35 Product description: Grilon TSG-35/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® XE 4174 black 9992 PA1010-GF30 Product description: Grilamid XE 4174 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 1010 injection molding grade. The main features of Grilamid XE 4174 black 9992 are: PA1010.. |
|||
Ball Indentation Hardness | 115 MPa @Time 30.0 sec |
16700 psi @Time 0.00833 hour |
DIN 53 456 |
Hippe PBT Polybutylene Terephthalate The mechanical properties of PBT are generally inferior to the partially crystallized PET, however, PBT is more easily machined.Information provided by Hippe. |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | H358/30; ISO 2039-1 |
Chi Mei Polylac® PA-707 ABS High gloss, high rigid |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | ISO 2039/1 |
BASF Ultramid® 1C PA6/66 (Conditioned) Description: Ultramid® 1C forms flexible, scratch-resistant coatings or tough, resilient, abrasion-resistant coverings on plastics, films, nonwovens, fabrics, leather, paper, wood, or metal.Informa.. |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | ISO 2039/1 |
BASF Ultramid® 1C PA6/66 (Dry) Description: Ultramid® 1C forms flexible, scratch-resistant coatings or tough, resilient, abrasion-resistant coverings on plastics, films, nonwovens, fabrics, leather, paper, wood, or metal.Informa.. |
|||
Ball Indentation Hardness | 115 MPa | 16700 psi | ISO 2039-1 |
Quadrant EPP Quadrant PSU unfilled, extruded (ISO Data) Quadrant 1000 PSU is a slightly yellow, translucent (non-optical quality) amorphous thermoplastic material, offering a combination of excellent mechanical, thermal and electrical properties. It ofte.. |