Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 36.2 - 36.2 J | 26.7 - 26.7 ft-lb | Average value: 36.2 J Grade Count:8 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Gardner Impact | 11.0 - 36.2 J | 8.11 - 26.7 ft-lb | Average value: 21.7 J Grade Count:5 |
Overview of materials for Epoxy Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Gardner Impact | 5.65 - 36.2 J | 4.17 - 26.7 ft-lb | Average value: 23.8 J Grade Count:17 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Gardner Impact | 2.71 - 36.2 J | 2.00 - 26.7 ft-lb | Average value: 18.2 J Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Gardner Impact | 36.0 - 36.2 J | 26.6 - 26.7 ft-lb | Average value: 36.1 J Grade Count:7 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Gardner Impact | 14.9 - 36.2 J | 11.0 - 26.7 ft-lb | Average value: 32.9 J Grade Count:25 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Gardner Impact | 36.2 - 36.2 J | 26.7 - 26.7 ft-lb | Average value: 36.2 J Grade Count:10 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Gardner Impact | 4.63 - 36.2 J | 3.42 - 26.7 ft-lb | Average value: 28.3 J Grade Count:4 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Gardner Impact | 1.40 - 36.2 J | 1.03 - 26.7 ft-lb | Average value: 20.6 J Grade Count:6 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |