Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 120 MPa | 17400 psi | ASTM D695 |
Chevron Phillips Ryton® R10 5004A PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Compressive Yield Strength | 120 MPa | 17400 psi | ISO 14126 |
Menzolit Menzolit® SMC 1100 Unsaturated Polyester UP SMC 1100 is a special vinylester SMC for high strength applications. The reinforcement has been put to a level that combines mouldability with high strength and stiffness properties. The specific re.. |
|||
Compressive Yield Strength | 120 MPa | 17400 psi | |
Sawbones E-Glass-Filled Epoxy Sheets Primary UseE-glass-filled epoxy sheets are primarily used as an alternative test medium to human cortical bone.DescriptionE-glass-filled epoxy sheets are a mixture of short e-glass fibers and epoxy .. |
|||
Compressive Yield Strength | 120 MPa | 17400 psi | |
Sawbones Third-Generation Simulated Cortical Bone E-glass-filled EpoxySawbones® Third-Generation Bones model natural cortical bone using a mixture of short e-glass fibers and epoxy resin pressure injected around a foam core. The mid-shaft area h.. |
|||
Compressive Yield Strength | 120 MPa | 17400 psi | |
Sawbones E-Glass-Filled Epoxy Cylinders Primary UseE-glass-filled epoxy cylinders are primarily used as an alternative test medium to human cortical bone.DescriptionThey are a mixture of short e-glass fibers and epoxy resin that has been .. |
|||
Compressive Yield Strength | >= 120 MPa | >= 17400 psi | Graphite substrate |
Destech Silicon Carbide, Solid or Foamed Destech silicon carbide foam is produced by chemical vapor reaction (CVR), in which high temperature silicon bearing gases convert glassy, or vitreous, carbon foam to SiC. Destech SiC foam has no c.. |
|||
Compressive Yield Strength | 120 - 1000 MPa | 17400 - 145000 psi | Average value: 292 MPa Grade Count:57 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |