Material Notes:
E-glass-filled EpoxySawbones® Third-Generation Bones model natural cortical bone using a mixture of short e-glass fibers and epoxy resin pressure injected around a foam core. The mid-shaft area has an intermedullarly canal.Third-generation composite bone was developed to improve the composite bone physical behavior, increase anatomical detail in the cortical wall and ease manufacturing difficulties of the Second-Generation Bone.Information provided by Sawbones.
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 90.0 MPa
13100 psi
Modulus of Elasticity 12.4 GPa
1800 ksi
Compressive Yield Strength 120 MPa
17400 psi
Compressive Modulus 7.60 GPa
1100 ksi