Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 82.7 MPa | 12000 psi | TM R050-38 |
Resinlab® EP1285HD-9 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Compressive Yield Strength | 83.0 MPa | 12000 psi | ASTM D695 |
Protective Coating PC-Crete™ Epoxy Putty PC-PUTTIES™ are hand moldable epoxy putty that are especially designed for emergency type repairs where time is of the essence.Data provided by the manufacturer. |
|||
Compressive Yield Strength | 83.0 MPa | 12000 psi | ASTM D695 |
Protective Coating PC-Lumber™ Epoxy Putty PC-PUTTIES™ are hand moldable epoxy putty that are especially designed for emergency type repairs where time is of the essence.Data provided by the manufacturer. |
|||
Compressive Yield Strength | 83.0 MPa | 12000 psi | ASTM D695 |
Protective Coating PC-Marine™ Epoxy Putty PC-PUTTIES™ are hand moldable epoxy putty that are especially designed for emergency type repairs where time is of the essence.Data provided by the manufacturer. |
|||
Compressive Yield Strength | 82.7 MPa | 12000 psi | ASTM D695 |
Protective Coating PC-Plumbing Epoxy Putty™ Hand Moldable, Multi-Purpose Epoxy Putty Stick Description: After Mixing, PC-Plumbing™ can be used to repair split and leaking pipes, tanks, drums, castings, ducts, valves and tools. It can be used wherever metal is missing, dented, broken, or .. |
|||
Compressive Yield Strength | 82.7 MPa | 12000 psi | TM R050-38 |
Resinlab® EP1320 Heat Cure Epoxy Conformal Coating Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the.. |
|||
Compressive Yield Strength | 82.7 - 121 MPa | 12000 - 17500 psi | Average value: 103 MPa Grade Count:4 |
Overview of materials for Polystyrene, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Compressive Yield Strength | 82.7 MPa | 12000 psi | ASTM D695 |
Fibre Glast 1099 Room Temperature Epoxy Surface Coat Safety hardener with fast overnight cure. Low viscosity thins the resin well for best detail reproduction. Can be sanded in 16-18 hours. #1099 is a white, medium viscosity epoxy surface coat that c.. |
|||
Compressive Yield Strength | 82.8 MPa | 12000 psi | |
Inchem Phenoxy PKFE Phenoxy PKFE - polyhydroxy ether of Bisphenol A. Originally developed by Union Carbide. Produced by InChem Corporation. |
|||
Compressive Yield Strength | 83.0 MPa | 12000 psi | |
Ineos Barex® 210 E Acrylonitrile-Methyl Acrylate Copolymer Extrusion Grade. Barex® Resins are available in either natural or blue tint. Barex® 210E is most commonly used for thermoformed sheet applications. |
|||
Compressive Yield Strength | 83.0 MPa @Strain 10.0 %, Temperature 23.0 °C |
12000 psi @Strain 10.0 %, Temperature 73.4 °F |
EN ISO 604 |
Ensinger TECASINT 3022 Polyimide, Black, 15% Graphite (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Compressive Yield Strength | 82.7 MPa | 12000 psi | ASTM D695 |
Devcon Magic Bond™ Epoxy Putty Emergency Repair ProductsComments: Two-part epoxy putty stick seals leaks and repairs gouges in steel, aluminum, wood, fiberglass, concrete and ceramics. Cures rock-hard and can be painted, sanded,.. |
|||
Compressive Yield Strength | 82.74 MPa | 12000 psi | |
Abatron AboCast/AboCure 8109-4 Safety hardener (minimum toxicity) version of 8109-3.Processing: 100/10 pbw; Potlife: 2.5 h/20°C (68°F), 30 min/40°C (105°F), 15 min/60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 .. |
|||
Compressive Yield Strength | 83.0 MPa | 12000 psi | ASTM D695 |
Protective Coating PC-Metal™ Epoxy Putty PC-PUTTIES™ are hand moldable epoxy putty that are especially designed for emergency type repairs where time is of the essence.Data provided by the manufacturer. |
|||
Compressive Yield Strength | 82.7 MPa | 12000 psi | ASTM D695 |
Adell HI-10 Impact Modified PBT |