Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Plaskolite Mustang PETG Sheet MUSTANG sheet signage material is continually processed using Eastman Tritan® copolyester, MUSTANG offers superior forming details, improved material distribution and shorter heating and cooling cy.. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Polymer Resources ABS-G5-[color]-3 ABS, 5% Glass Reinforced, UV-stabilized Acrylonitrile Butadiene Styrene, 5% Glass Reinforced, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Polymer Resources TP-FR-IM2 Polybutylene Terephthalate, Impact Modified, Flame Retardant, High Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Polymer Resources TP-FR-IM2-[color]-6 Polybutylene Terephthalate, Low Temperature Impact Modified, Flame Retardant Polybutylene Terephthalate, Low Temperature Impact Modified, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t.. |
|||
Flexural Strength | 65.5 MPa @Thickness 3.17 mm |
9500 psi @Thickness 0.125 in |
ASTM D790 |
PTS Trilac® FR3800 Flame Retardant ABS Resin, RoHS Compliant Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
PolyOne Stat-Tech™ AS-10SS/000 ABS - 10% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Fiberfil® J-60/10 Polypropylene Homopolymer, 10% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 65.5 MPa | 9500 psi | |
Malvern Minerals Diallylphthalate with Untreated Novacite® 1250 Quartz Filler Product data demonstrates the effect of the Novacite® quartz filler. Separate entries demonstrate the effect of silane-treated Novakup® quartz filler in DAP. The specific DAP used is Dapon 3.. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Techmer ES Elastoblend® PA6 IM L W Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Techmer ES Elastoblend® PA6 IM L W N Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Techmer ES Elastoblend® PA6 IM X Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedProcessing Method: Injection MoldingInformat.. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Techmer ES Plastiblend® PA6/ABS 1120 B1 Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Techmer ES Plastiblend® PBT/ABS BK Availability: North AmericaForms: PelletsAppearance: BlackTPCI# 6722121Information provided by TP Composites, Inc. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Techmer ES HiFill FR® PA6 FR-N IM Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Flame Retardant, Heat Stabilized, Impact Modified, Halogen Free and Lubricated Appearance: .. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Ecomass® 1700CO93 Copper Powder Filled Polyamide, Injection Molding High Specific Gravity, Copper Powder Filled Polyamide (PA), Rigid, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting and balancing applicationsInform.. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Adell ZS-30 Nylon/Olefin Alloy Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790-95 |
Multibase Multi-ABS 3246 High Flow Grade Data provided by Multibase. |